Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Panlite® L-1225L - PC - Teijin Chemicals Ltd.

Material Data Center offers the following functions for Panlite® L-1225L:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Panlite datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 18 cm³/10min ISO 1133
Température 300 °C -
Charge 1.2 kg -
ASTM Data
Retrait au moulage , parallèle 0.006 mm/mm ASTM D 955
Retrait au moulage, perpendiculaire 0.006 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2400 MPa ISO 527
Contrainte d'écoulement 61 MPa ISO 527
Déformation au seuil d'écoulement 6 % ISO 527
Déformation nominale à la rupture >50 % ISO 527
Module de flexion, 23°C 2350 MPa ISO 178
Résistance à la flexion 93 MPa ISO 178
Résistance au choc Charpy, +23°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 67 kJ/m² ISO 179/1eA
ASTM Data
Module en traction 2170 MPa ASTM D 638
Module de traction d’élasticité 63 MPa ASTM D 638
Résistance de traction à la rupture 74 MPa ASTM D 638
Allongement d’élasticité 6 % ASTM D 638
Allongement à la rupture 140 % ASTM D 638
Résistance de compression 77 MPa ASTM D 695
Module de flexion 2280 MPa ASTM D 790
Résistance à la flexion 90 MPa ASTM D 790
Dureté Rockwell M 77 - ASTM D 785
Izod choc avec entaille, 1/8 in 780 J/m ASTM D 256
Izod choc avec entaille, 1/4 in 100 J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 126 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 139 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 146 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 70 E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 70 E-6/K ISO 11359-1/-2
Inflammabilité pr. épaisseur h V-2 class IEC 60695-11-10
Epaisseur de l'éprouvette 0.4 mm -
Glow Wire Flammability Index (GWFI) 850 °C IEC 60695-2-12
GWFI - thickness tested (1) 1.5 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 3 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (1) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (2) 3 mm -
ASTM Data
UL 94 inflammabilité HB - UL 94
Épaisseur testée 1.9 mm -
coefficient de dilatation thermique, long. 70 E-6/K ASTM D 696
Coefficient de dilatation thermique, trav. 70 E-6/K ASTM D 696
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 3.1 - IEC 62631-2-1
Permittivité relative, 1MHz 3 - IEC 62631-2-1
Facteur de pertes, 100Hz 10 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 90 E-4 IEC 62631-2-1
Résistivité transversale >1E13 Ohm*m IEC 62631-3-1
Résistivité superficielle >1E15 Ohm IEC 62631-3-2
Rigidité diélectrique 30 kV/mm IEC 60243-1
Indice de résistance au cheminement 250 - IEC 60112
ASTM Data
Rigidité diélectrique, peu de temps 30 kV/mm ASTM D 149
Facteur de dissipation diélectrique, 60 Hz 0.0004 - ASTM D 150
Facteur de dissipation diélectrique, 1 MHz 0.009 - ASTM D 150
Constante diélectrique, 60 Hz 2.95 - ASTM D 150
Constante diélectrique, 1 MHz 2.9 - ASTM D 150
Résistance volumique 3E16 Ohm*cm ASTM D 257
Résistance à l’arc 110 s ASTM D 495
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Lumière á Transmittance 88 % ASTM D 1003
Indice de réfraction 1.58 - ASTM D 542
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1200 kg/m³ ISO 1183
Absorption d’eau, équilibre 0.2 % ASTM D 570
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 120 °C -
Pré-séchage - temps >5 h -
Température de la matière fondue 270 - 320 °C -
Température du moule 80 - 120 °C -
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Additifs
Agent de démoulage
Propriétés spéciales
Transparent
Applications
Automobile, General Purpose
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.