Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pebax® MV 1074 SP 01 - TPA - ARKEMA

Material Data Center offers the following functions for Pebax® MV 1074 SP 01:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Pebax datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Polyether block amide Pebax® MV 1074 SP 01 resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide.
Pebax® MV 1074 SP 01 resin is an inherently dissipative polymer and can be dry blended or compounded with an isolative polymer to lower the surface resistivity. This hydrophilic grade when extruded into either a thin film or laminated on to a substrate offers excellent permeability to moisture vapor while remaining waterproof.
This SP grade has been developed to be heat and UV resistant.

Refractive index according to an internal method is 1.502.


Main applications:
  • Breathable membranes
  • Permanent antistactic additive


Packaging:

This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 97 / 80 MPa ISO 527
Contrainte pr. une déform. de 50% 10 / 10 MPa ISO 527
Déformation à la rupture >50 / >50 % ISO 527
Contrainte à la rupture TPE 30 / * MPa ISO 527
Déformation à la rupture TPE >300 / * % ISO 527
Dureté Shore D 38 / * - ISO 7619-1
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 158 / * °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min -40 / * °C ISO 11357-1/-2
Aptitude à l'allumage 19 / * % ISO 4589-1/-2
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Résistivité transversale 1.5E9 / 2.5E7 Ohm*m IEC 62631-3-1
Résistivité superficielle * / 3E9 Ohm IEC 62631-3-2
Rigidité diélectrique 5 / - kV/mm IEC 60243-1
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 48 / * % Sim. to ISO 62
Absorption d'humidité 1.4 / * % Sim. to ISO 62
Masse volumique 1070 / - kg/m³ ISO 1183
Propriétés mécaniques (Grades film)sec / condUnitéNorme du test
ISO Data
Contrainte maximale, parallèle 32 / * MPa ISO 527-3
Contrainte maximale, perpend. 34 / * MPa ISO 527-3
Déformation maximale, parallèle 500 / * % ISO 527-3
Déformation maximale, perpend. 700 / * % ISO 527-3
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 65 - 75 °C -
Pré-séchage - temps 4 - 6 h -
Température de la matière fondue 200 - 270 °C -
Température du moule 25 - 60 °C -
Fonctions
Viscosité / Vitesse de cisaillement , Pebax® MV 1074 SP 01, TPA, ARKEMA
Contrainte de cisaillement / Vit. de cisaillement , Pebax® MV 1074 SP 01, TPA, ARKEMA
Contrainte / Déformation , Pebax® MV 1074 SP 01 (sec), TPA, ARKEMA
Module sécant / Déformation , Pebax® MV 1074 SP 01 (sec), TPA, ARKEMA
Caractéristiques
Transformation
Moulage par injection, Extrusion de films, Extrusion de profilés, Extrusion (autres), Moulage par transfert, Coulage, Thermoformage
Conditionnement
Granulés
Propriétés spéciales
Conductivité électrique accrue, Antistatique, Stabilisé à la lumière, Stabilisé aux intempéries, Stabilisé à la chaleur
Disponibilité régionale
Autres informations
Moulages par injection

Processing conditions:

- Typical melt temperature (Min / Recommended / Max): 200°C / 240°C / 270°C.
- Typical mold temperature: 25–60°C.
- Drying time and temperature (only necessary for bags opened for more than two hours): 4-6 hours at 65-75°C.
Extrusion (autres)

Processing conditions:

- Typical melt temperature (Min / Recommended / Max): 210°C / 220°C / 230°C.
- Drying time and temperature (only necessary for bags opened for more than two hours): 4-6 hours at 65-75°C.
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com