Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pebax® Rnew® 80R53 SP 02 - TPA - ARKEMA

Material Data Center offers the following functions for Pebax® Rnew® 80R53 SP 02:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Pebax datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Polyether block Pebax® Rnew ® 80R53 SP 02 resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV resistant.

According to ASTM D6866, the biobased carbon content is measured at 92%.



Main applications:
  • Ski shoes
  • Athletic foot wear components


Packaging:

This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction - / 944 MPa ISO 527
Contrainte d'écoulement - / 33 MPa ISO 527
Déformation au seuil d'écoulement - / 24 % ISO 527
Déformation nominale à la rupture - / >50 % ISO 527
Résistance au choc Charpy (entaillé), +23°C - / 44 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C - / 16 kJ/m² ISO 179/1eA
Dureté Shore D 67 / * - ISO 7619-1
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 188 / * °C ISO 11357-1/-3
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 0.7 / * % Sim. to ISO 62
Absorption d'humidité 0.8 / * % Sim. to ISO 62
Masse volumique 1020 / 1020 kg/m³ ISO 1183
Biobased content 89 % -
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 70 - 80 °C -
Pré-séchage - temps 5 - 7 h -
Température de la matière fondue 230 - 260 °C -
Température du moule 25 - 60 °C -
Fonctions
Contrainte / Déformation , Pebax® Rnew® 80R53 SP 02 (cond.), TPA, ARKEMA
Module sécant / Déformation , Pebax® Rnew® 80R53 SP 02 (cond.), TPA, ARKEMA
Caractéristiques
Transformation
Moulage par injection, Extrusion (autres)
Conditionnement
Granulés
Propriétés spéciales
Stabilisé à la lumière, Stabilisé aux intempéries, Stabilisé à la chaleur
Certifications
Contient des ressources renouvelables
Disponibilité régionale
Autres informations
Moulages par injection

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 230°C / 260°C / 290°C.
- Typical mold temperature : 25 – 60°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 5-7 hours at 70-80°C.

Extrusion (autres)

Processing conditions:

- Typical melt temperature (Min / Recommended / Max): 230°C / 260°C / 290°C.
- Drying time and temperature (only necessary for bags opened for more than two hours): 5-7 hours at 70-80°C.
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.