Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Platamid® H 106 Powder - PA* - ARKEMA

Material Data Center offers the following functions for Platamid® H 106 Powder:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Platamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Platamid® H 106 Powder
Copolyamide Hot Melt Adhesive / Textile Applications

Platamid® H 106 Powderis a very low melt copolyamide adhesive powder for the production of fusible interlinings. Platamid® H 106 Powder is particularly useful where bonding temperature low and short bonding time are required for sensitive shell fabrics.
Platamid® H 106 Powder has an excellent dry cleaning resistance and washing resistance up to 40°C.

AVAILABLE GRADES
This product is available in different grain sizes:
- Platamid® H 106 PA 100
- Platamid® H 106 PA 80 (0-80 μm)
- Platamid® H 106 PRA 200/25 (0-200 μm)
- Platamid® H 106 PTA 120 (0-120 μm)
- Platamid® H 106 PTA 170 (80-170 μm)
- Platamid® H 106 PTA 170/20 (0-70 μm)
- Platamid® H 106 PA 80 Black
- Platamid® H 106 PA 80 Red
- Platamid® H 106 PRA 170
- Platamid® H 106 PTA 170 Black
- Platamid® H 106 PTA 170 Red
- Platamid® H 106 PTA 60/150
 
PACKAGING
All grades are delivered in 20 kg sealed bags.
Platamid® H 106 PA 80 is also delivered in 500 kg sealed big bags (GRVS).
These grades are ready to be processed.
 
SHELF LIFE
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 90 / * cm³/10min ISO 1133
Température 160 / * °C -
Charge 2.16 / * kg -
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 115 / * °C ISO 11357-1/-3
Caractéristiques
Conditionnement
Poudre
Caractéristiques
Copolymère
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.