Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Platamid® HX 2544 Powder - PA* - ARKEMA

Material Data Center offers the following functions for Platamid® HX 2544 Powder:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Platamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Platamid® HX 2544 Powder
Copolyamide Hot Melt Adhesive / Textile Applications

Platamid® HX 2544 Powder is a low melt viscosity copolyamide adhesive powder for the production of fusible interlinings.
Platamid® HX 2544 Powder is particularly useful where low and short bonding conditions are required for leather and fur.
Platamid® HX 2544 Powder has good dry cleaning resistance and washing resistance up to 60°C.
Platamid® HX 2544 Powder has a renewable carbon content of 60% (internal method).


AVAILABLE GRADES
This grade is available in different grain sizes:
- Platamid® HX 2544 PA80 (0-80 µm paste dot)
- Platamid® HX 2544 PTA 170 (80-170 µm double dot)
- Platamid® HX 2544 PRA 170 (80-170 µm double dot)
PACKAGING
- Platamid®HX 2544 Powder is delivered in 25 kg sealed bags.
SHELF LIFE
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
RENEWABLE CARBON CONTENT
60% (internal method)
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 104 / * cm³/10min ISO 1133
Température 160 / * °C -
Charge 2.16 / * kg -
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 95 / * °C ISO 11357-1/-3
Propriétés diversesValeurUnitéNorme du test
Biobased content 60 % -
Caractéristiques
Conditionnement
Poudre
Caractéristiques
Copolymère
Certifications
Contient des ressources renouvelables
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.