Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Platamid® H 1937 Pellets - PA* - ARKEMA

Material Data Center offers the following functions for Platamid® H 1937 Pellets:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Platamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Platamid® H 1937 Pellets
Copolyamide Hot Melt Adhesive / Extrusion Applications

Platamid® H 1937 is a thermoplastic copolyamide adhesive available in pellet form for manufacture of hot melt film and webs by extrusion.

Platamid® H 1937 has good adhesion to all kinds of textile substrates based on native and synthetic fibers. 




AVAILABLE GRADES
This product is available:
- dried (H 1937 TA)
PACKAGING
- Platamid® H 1937 TA is delivered in 25 kg sealed bags.
This grade is ready to be processed.
SHELF LIFE
Two years from the date of delivery. For any use above this limit, please refer to our technical services.

Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 18 / * cm³/10min ISO 1133
Température 160 / * °C -
Charge 2.16 / * kg -
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 102 / * °C ISO 11357-1/-3
Caractéristiques
Transformation
Extrusion de films
Conditionnement
Granulés
Caractéristiques
Bonne adhérence, Copolymère
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.