Caractéristiques des transformations/physiques | Valeur | Unité | Norme du test |
Other Standards[S] |
Indice de fluidité, MFI |
20 |
g/10min |
DIN 53735 |
Température |
220 |
°C |
- |
Charge |
10 |
kg |
- |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés mécaniques | Valeur | Unité | Norme du test |
ISO Data |
Résistance au choc Charpy (entaillé), +23°C |
10 |
kJ/m² |
ISO 179/1eA |
Résistance au choc Izod avec entaille, +23°C |
17 |
kJ/m² |
ISO 180/1A |
Other Standards[S] |
Module en traction |
2400 |
MPa |
DIN 53457 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés thermiques | Valeur | Unité | Norme du test |
Other Standards[S] |
Température de ramolliss. Vicat, B |
95 |
°C |
DIN 53460 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés diverses | Valeur | Unité | Norme du test |
Other Standards[S] |
Masse volumique |
1060 |
kg/m³ |
DIN 53479 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Caractéristiques
Conditionnement
Noir
Disponibilité régionale
Europe
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.