Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Provista™ ST - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Provista™ ST:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Provista datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

Eastman Provista™ Copolymer ST is a resin specifically developed for profile extrusion where high clarity and gloss, toughness, and processability are critical. Eastman Provista™ Copolymer ST is a second-generation material that complements Eastman Provista™ by offering similar features, while providing greater toughness. Eastman Provista™ Copolymer ST is ideal in applications that place greater physical demands on the profile. Eastman Provista™ Copolymer ST is certified to NSF/ANSI Standard 51 for Food Equipment Materials.




Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Retrait au moulage , parallèle 0.003 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ASTM Data
Module en traction 1900 MPa ASTM D 638
Module de traction d’élasticité 47 MPa ASTM D 638
Résistance de traction à la rupture 48 MPa ASTM D 638
Allongement d’élasticité 5 % ASTM D 638
Allongement à la rupture 300 % ASTM D 638
Module de flexion 1900 MPa ASTM D 790
Résistance à la flexion 65 MPa ASTM D 790
Dureté Rockwell R 105 - ASTM D 785
Izod choc avec entaille, 1/8 in N J/m ASTM D 256
Izod choc avec entaille, bas température 63 J/m ASTM D 256
Température -40 °C -
Résistance au choc Izod, 1/8 in N J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
DTUL à 66 psi 73 °C ASTM D 648
DTUL à 264 psi 63 °C ASTM D 648
Vicat température 85 °C ASTM D 1525
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Brillant 143 - ASTM D 2457
Haze 1.3 % ASTM D 1003
Lumière á Transmittance 91 % ASTM D 1003
Propriétés diversesValeurUnitéNorme du test
Densité 1250 kg/m³ ASTM D 792
Caractéristiques
Transformation
Extrusion de profilés
Propriétés spéciales
Transparent
Caractéristiques
High Gloss, Copolymère
Résistance Chimique
Résistance chimique générale
Certifications
Contact alimentaire, FDA 21 CFR approbation
Applications
Emballage
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.