Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsamid® AMNO P40 TLD - PA12 - ARKEMA

Material Data Center offers the following functions for Rilsamid® AMNO P40 TLD:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Rilsamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
PA12-P, MHLR, 12-004
Rilsamid® AMNO P40 TLD resin is a natural polyamide. This grade is plasticized and designed for injection molding.
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 51 / * cm³/10min ISO 1133
Température 235 / * °C -
Charge 2.16 / * kg -
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 440 / 420 MPa ISO 527
Contrainte d'écoulement 26 / 24 MPa ISO 527
Déformation au seuil d'écoulement 26 / 26 % ISO 527
Déformation nominale à la rupture >50 / >50 % ISO 527
Résistance au choc Charpy (entaillé), +23°C - / 25 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C - / 4 kJ/m² ISO 179/1eA
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 171 / * °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 46 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 125 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 132 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 140 / * E-6/K ISO 11359-1/-2
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 12 / - - IEC 62631-2-1
Permittivité relative, 1MHz 4 / - - IEC 62631-2-1
Facteur de pertes, 100Hz 2550 / - E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 1290 / - E-4 IEC 62631-2-1
Résistivité transversale - / 1E9 Ohm*m IEC 62631-3-1
Résistivité superficielle * / 5E11 Ohm IEC 62631-3-2
Rigidité diélectrique - / 24 kV/mm IEC 60243-1
Indice de résistance au cheminement * / 600 - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 1.2 / * % Sim. to ISO 62
Masse volumique 1040 / 1040 kg/m³ ISO 1183
Fonctions
Viscosité / Vitesse de cisaillement , Rilsamid® AMNO P40 TLD, PA12, ARKEMA
Contrainte de cisaillement / Vit. de cisaillement , Rilsamid® AMNO P40 TLD, PA12, ARKEMA
Contrainte / Déformation (isochrone) 23°C, Rilsamid® AMNO P40 TLD (sec), PA12, ARKEMA
Module de fluage / Temps 23°C, Rilsamid® AMNO P40 TLD (sec), PA12, ARKEMA
Courbe de fluage 23°C, Rilsamid® AMNO P40 TLD (sec), PA12, ARKEMA
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Additifs
Agent de démoulage, Plastifiant
Propriétés spéciales
Stabilisé à la lumière, Stabilisé aux intempéries, Stabilisé à la chaleur
Disponibilité régionale
Autres informations
Moulages par injection

Processing conditions, Injection:

- Typical melt temperature (Min / Recommended / Max) : 230°C / 250°C / 270°C.
- Mold temperature : 20 - 40°C
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 80 - 90°C.
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.