Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsamid ® AZM 50 BLACK T6LD - PA12-GF50 - ARKEMA

Material Data Center offers the following functions for Rilsamid ® AZM 50 BLACK T6LD:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Rilsamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
ISO 16396 - PA12, GF50, M1GHLR, C16-120

Rilsamid® AZM 50 BLACK T6LD resin is a fiberglass reinforced polyamide. 
This black colored grade is designed for injection molding.




Packaging : 
This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed

Shelf life : 
Two years from the delivery.
For any use above this limit please refer to our technical services. 
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 6 / * cm³/10min ISO 1133
Température 235 / * °C -
Charge 5 / * kg -
Retrait au moulage, parallèle 0.2 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.7 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 12000 / 12100 MPa ISO 527
Contrainte à la rupture 152 / 144 MPa ISO 527
Déformation à la rupture 4.6 / 4.9 % ISO 527
Résistance au choc Charpy, +23°C 84 / 80 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 90 / 84 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 22 / 21 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 15 / 15 kJ/m² ISO 179/1eA
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 175 / * °C ISO 11357-1/-3
Propriétés diversessec / condUnitéNorme du test
Masse volumique 1470 / - kg/m³ ISO 1183
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Grains, Noir
Additifs
Agent de démoulage
Propriétés spéciales
Stabilisé à la lumière, Stabilisé à la chaleur
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America
Autres informations
Moulages par injection

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 250°C / 265°C / 280°C.
- Typical mold temperature : 40 – 90°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-8 hours at 80-90°C.

Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.