Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® HT CZM 30 BLACK TLD - PA*-GF30 - ARKEMA

Material Data Center offers the following functions for Rilsan® HT CZM 30 BLACK TLD:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
PA11/10T,GF30,MHL,C16-090  

Rilsan® HT CZM 30 BLACK TLD is a polyphthalamide produced from a renewable source. This grade is glass fiber-reinforced, formulated and designed for injection molding for high-temperature applications.

According to ASTM D6866, the biobased carbon content is measured at 68%.



Main applications:
  • Automotive & transportation quick connector for flexible fuels and powertrain applications
  • High-temperature injection molding

Packaging:
This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit,  please refer to our technical services.
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 15 / * cm³/10min ISO 1133
Température 300 / * °C -
Charge 2.16 / * kg -
Retrait au moulage, parallèle 0.3 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.0 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 8700 / - MPa ISO 527
Contrainte à la rupture 151 / - MPa ISO 527
Déformation à la rupture 2.6 / - % ISO 527
Résistance au choc Charpy, +23°C 57 / - kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 54 / - kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 9.1 / - kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 7.4 / - kJ/m² ISO 179/1eA
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 255 / * °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 220 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 240 / * °C ISO 75-1/-2
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 1.13 / * % Sim. to ISO 62
Absorption d'humidité 0.22 / * % Sim. to ISO 62
Masse volumique 1300 / 1300 kg/m³ ISO 1183
Biobased content 67 % -
Fonctions
Viscosité / Vitesse de cisaillement , Rilsan® HT CZM 30 BLACK TLD, PA*-GF30, ARKEMA
Contrainte de cisaillement / Vit. de cisaillement , Rilsan® HT CZM 30 BLACK TLD, PA*-GF30, ARKEMA
Contrainte / Déformation , Rilsan® HT CZM 30 BLACK TLD (sec), PA*-GF30, ARKEMA
Module sécant / Déformation , Rilsan® HT CZM 30 BLACK TLD (sec), PA*-GF30, ARKEMA
Volume spécifique (pvT) , Rilsan® HT CZM 30 BLACK TLD, PA*-GF30, ARKEMA
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés, Noir
Additifs
Agent de démoulage
Propriétés spéciales
Stabilisé à la lumière, Stabilisé aux intempéries, Stabilisé à la chaleur
Certifications
Contient des ressources renouvelables
Disponibilité régionale
Autres informations
Moulages par injection
Injection molding process conditions :
- Typical melt temperature (Min / Recommanded / Maxi) : 270°C  / 280°C / 320°C.
- Typical mold temperature : 90 - 110°C.
- Drying time and temperature (only for bags opened for more than two hours) : 4 - 8 hours / 100 - 110°C.
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.