Scanamid 6 - PA6 - Polykemi AB

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Scanamid 6" in Material Data Center leads to the following information:

Tradename: Scanamid 6
Family: PA6
Producer: Polykemi AB
80 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
SCANAMID 6 B11^ PA6
SCANAMID 6 B11^ F30 PA6-GF30
SCANAMID 6 B11^ F30 FR5 PA6-GF30
SCANAMID 6 B11^ F45 PA6-GF45
SCANAMID 6 B11^ F50 PA6-GF50
SCANAMID 6 B11^ FX25 FR10 PA6-GF25
SCANAMID 6 B11^FC PA6
SCANAMID 6 B12^ PA6
SCANAMID 6 B12^ F PA6
SCANAMID 6 B12^ F15 PA6-GF15
SCANAMID 6 B12^ F20 PA6-GF20
SCANAMID 6 B12^ F20 NH6 PA6-GF20
SCANAMID 6 B12^ F25 PA6-GF25
SCANAMID 6 B12^ F25 FR6 PA6-GF25
SCANAMID 6 B12^ F30 PA6-GF30
SCANAMID 6 B12^ F30 AS PA6-GF30
SCANAMID 6 B12^ F40 PA6-GF40
SCANAMID 6 B12^ F45 PA6-GF45
SCANAMID 6 B12^ F50 PA6-GF45
SCANAMID 6 B12^ FX30 PA6-GF30
SCANAMID 6 B12^ NH11L PA6
SCANAMID 6 B12^ NH6 PA6
SCANAMID 6 B12^ NH9 PA6
SCANAMID 6 B12^ NH9L PA6
SCANAMID 6 B12^ Q40 PA6-MX40
SCANAMID 6 B12^ QF2010 PA6-GF30
SCANAMID 6 B12^ QF2515 PA6-(GF+MX)40
SCANAMID 6 B12^ FC PA6
SCANAMID 6 B13^F30 PA6-GF30
SCANAMID 6 B22^E F15 PA6-GF15
SCANAMID 6 B22^E F20 PA6-GF20
SCANAMID 6 B22^E F30 PA6-GF30
SCANAMID 6 B22^E F40 PA6-GF40
SCANAMID 6 B23^E F30 PA6-GF30
SCANAMID 6 B32^E PA6
SCANAMID 6 B32^E F15 PA6-GF15
SCANAMID 6 B32^E F30 PA6-GF30
SCANAMID 6 B32^E Q30 PA6-MX30
SCANAMID 6 B32^EF F15 PA6-GF15
SCANAMID 6 B33^E F15 PA6-GF15
SCANAMID 6 B43^D F15 PA6-GF15
SCANAMID 6 B52^E PA6
SCANAMID 6 B60 PA6-MX60
SCANAMID 66 A11^ X30 PA66-GX30
SCANAMID 66 A11^ X30 LS PA66-GX30
SCANAMID 66 A12^ PA66
SCANAMID 66 A12^ F12 PA66-GF12
SCANAMID 66 A12^ F15 PA66-GF15
SCANAMID 66 A12^ F20 PA66-GF20
SCANAMID 66 A12^ F20 FR6 PA66-GF20
SCANAMID 66 A12^ F25 FR6 PA66-GF25
SCANAMID 66 A12^ F25 NH10 PA66-GF25
SCANAMID 66 A12^ F30 PA66-GF30
SCANAMID 66 A12^ F30 TF15 PA66-GF30
SCANAMID 66 A12^ F35 PA66-GF35
SCANAMID 66 A12^ F35 NH9 PA66-GF35
SCANAMID 66 A12^ F50 PA66-GF50
SCANAMID 66 A12^ Q40 PA66-MX40
SCANAMID 66 A12^ QF2515 PA66-(MX+GF)40
SCANAMID 66 A12^ X30 PA66-GX30
SCANAMID 66 A12^F PA66
SCANAMID 66 A12^FC PA66
SCANAMID 66 A13^ F15 PA66-GF15
SCANAMID 66 A13^ F30 PA66-GF30
SCANAMID 66 A13^ FX30 PA66-GF30
SCANAMID 66 A13^ Q2 EX8 PA66-MX18
SCANAMID 66 A32^E PA66
SCANAMID 66 A32^E Q30 PA66-MX30
SCANAMID 66 A33^E PA66
SCANAMID 66 A33^E F15 PA66-GF15
SCANAMID 66 A33^E F30 PA66-GF30
SCANAMID 66 A33^E F45 PA66-GF45
SCANAMID 66 A43^E F14 PA66-GF14
SCANAMID 66 A52^E PA66
SCANAMID 66 A53^ F43 PA66-GF43
SCANAMID 66 A53^E PA66
SCANAMID 66 A53^EM PA66
SCANAMID 66 AL220L2M PA66
SCANAMID 66.6 C12^ F30 PA666-GF30
SCANAMID 66.6 C22^E F PA666

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.