Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of STYRON™ 637 - PS - Trinseo

Material Data Center offers the following functions for STYRON™ 637:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Styron datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité, MFI 2.5 g/10min ISO 1133
Température 200 °C -
Charge 5 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Contrainte d'écoulement 55 MPa ISO 527
Déformation à la rupture 2 % ISO 527
Module de flexion, 23°C 3500 MPa ISO 178
Dureté Rockwell R105 - ISO 2039-2
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de ramolliss. Vicat, A 97 °C ISO 306
Température de ramolliss. Vicat, B 92 °C ISO 306
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 mm -
Propriétés électriquesValeurUnitéNorme du test
ASTM Data
Facteur de dissipation diélectrique, 1 MHz 6.0E-5 - ASTM D 150
Constante diélectrique, 1 MHz 2.5 - ASTM D 150
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1050 kg/m³ ISO 1183
Caractéristiques
Transformation
Moulage par injection, Extrusion (autres)
Caractéristiques
Moussable
Certifications
Contact alimentaire, Approuvé pour le contact alimentaire suivant 10/2011, FDA 21 CFR approbation
Applications
General Purpose, Emballage
Disponibilité régionale
Europe, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com