Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ FX100 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ FX100:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

Eastman Tritan™ FX100 is a copolyester resin for extruded film applications where enhanced heat resistance and toughness are required. It works great in high temperature packaging, transaction and identification cards, and

protective laminates.

Packaging brands and film converters prefer Tritan™ FX100 for its ability to provide a clear, aesthetically pleasing package that stands up to the strenuous requirements for hot filling, while also providing safety that consumers expect. It’s great for brands looking to replace materials of concern or premiumize their packaging by transitioning from opaque to clear.

Transaction and identification card producers, brands, and governments alike value Tritan™ FX100 for its excellent bend strength and chemical resistance, which provides longer useful life and better security. Compared to PVC and other material alternatives. Transaction cards made with Tritan™ have been found to withstand more than 10 times the number of flexural cycles using industry standard fitness for use testing protocols.

Tritan™ FX100 may be used in various food contact applications under the U.S. Food & Drug Administration (FDA) regulations.

Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
coefficient de dilatation thermique, long. 90 E-6/K ASTM D 696
Température de transition vitreuse 110 °C ASTM E 1356
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Brillant 161 - ASTM D 2457
Haze 0.7 % ASTM D 1003
Lumière á Transmittance 92 % ASTM D 1003
Indice de réfraction 1.55 - ASTM D 542
Propriétés diversesValeurUnitéNorme du test
Absorption d’eau, 24hr 0.5 % ASTM D 570
Densité 1190 kg/m³ ASTM D 792
Propriétés mécaniques (Grades film)ValeurUnitéNorme du test
ISO Data
Résistance au déchirement pantalon, parallèle 11 N/mm ISO 6383-1
Résistance au déchirement pantalon, normal 11 N/mm ISO 6383-1
Epaisseur des eprouvettes 0.254 mm -
ASTM Data
Module en traction, long. 1500 MPa ASTM D 882
Module en traction, trav. 1400 MPa ASTM D 882
Module de traction d’élasticité, long. 41 MPa ASTM D 882
Module de traction d’élasticité, trav. 40 MPa ASTM D 882
Résistance de traction à la rupture, long. 59 MPa ASTM D 882
Résistance de traction à la rupture, trav. 52 MPa ASTM D 882
Allongement d’élasticité, long. 7 % ASTM D 882
Allongement d’élasticité, trav. 7 % ASTM D 882
Allongement à la rupture, long. 179 % ASTM D 882
Allongement à la rupture, trav. 203 % ASTM D 882
Epaisseur des eprouvettes 0.254 mm -
Caractéristiques
Transformation
Extrusion (autres)
Propriétés spéciales
Stabilisé à la chaleur, Transparent
Caractéristiques
Amorphe, High Gloss, Résistant aux rayures, Copolymère
Résistance Chimique
Résistance chimique générale
Certifications
Contact alimentaire, FDA 21 CFR approbation
Applications
Emballage
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com