Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TROGAMID® myCX high flow - PAPACM12 - Evonik Operations GmbH

Material Data Center offers the following functions for TROGAMID® myCX high flow:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Trogamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Microcrystalline, permanently transparent polyamide

TROGAMID® myCX high flow is a microcrystalline transparent polyamide for the manufacture of parts in the optical industry, like lenses according the injection molding procedure. 

TROGAMID® myCX high flow is supplied as spherical pellets in moisture-proof packaging.

Pigmentation may affect values.

For information about processing of TROGAMID®, please follow the general commendations about “Processing of TROGAMID® compounds”. 
 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.TROGAMID.COM

Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 11 / * cm³/10min ISO 1133
Température 280 / * °C -
Charge 2.16 / * kg -
Retrait au moulage, parallèle 0.7 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.7 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 1480 / 1490 MPa ISO 527
Contrainte d'écoulement 59 / 63 MPa ISO 527
Déformation au seuil d'écoulement 8 / 7 % ISO 527
Déformation nominale à la rupture >50 / >50 % ISO 527
Résistance au choc Charpy, +23°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 11 / 12 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Résistance au choc Charpy (entaillé), -30°C 11 / 12 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Dureté Shore D 81 / * - ISO 7619-1
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 247 / * °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min 135 / * °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 102 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 120 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 127 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 92 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 96 / * E-6/K ISO 11359-1/-2
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 3 / * % Sim. to ISO 62
Absorption d'humidité 2 / * % Sim. to ISO 62
Masse volumique 1020 / - kg/m³ ISO 1183
Caractéristiques
Transformation
Moulage par injection, Extrusion de films, Extrusion (autres)
Conditionnement
Grains
Propriétés spéciales
Transparent
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.