Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of TYMAX™ GT7001 - EMA - Westlake Chemical Corp.
unit conversion, PDF datasheet print, comparison with other plastics
Check here, which other Tymax datasheets, application examples or technical articles are available in Material Data Center
Extrusion coating
Laminations
Tie-layer
TYMAX® GT7001 is a maleic anhydride modified ethylene methyl acrylate copolymer designed for use as a tie layer in extrusion coating and lamination applications. This resin is designed for bonding to polyolefins, polyamides, and PET in multilayer film structures. It does not contain any slip or antiblock additives.
This product has some 21 CFR clearances.
Caractéristiques des transformations/physiques | Valeur | Unité | Norme du test | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ASTM Data | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Indice de fluidité, MFI | 6 | g/10min | ASTM D 1238 |
Propriétés thermiques | Valeur | Unité | Norme du test | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ASTM Data | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Température de fusion | 84 | °C | ASTM D 3418 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Vicat température | 51 | °C | ASTM D 1525 |
Propriétés diverses | Valeur | Unité | Norme du test |
Densité | 942 | kg/m³ | ASTM D 792 |
Recommandations pour la transformation Extrusion | Valeur | Unité | Norme du test |
Température de la matière fondue | <330 | °C | - |