Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultradur® B 6550 LN - PBT - BASF

Material Data Center offers the following functions for Ultradur® B 6550 LN:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultradur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
High viscosity extrusion grade for loose-buffer tubes in fibre optical cable applications and for semi-finished products, profiles and tubes and sheet.

Abbreviated designation according to ISO 1043-1: PBT
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 9.5 cm³/10min ISO 1133
Température 250 °C -
Charge 2.16 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2600 MPa ISO 527
Contrainte d'écoulement 56 MPa ISO 527
Déformation au seuil d'écoulement 3.5 % ISO 527
Déformation nominale à la rupture >50 % ISO 527
Résistance au choc Charpy, +23°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 220 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 5 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 5 kJ/m² ISO 179/1eA
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 223 °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 50 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 135 °C ISO 75-1/-2
Coeffic. de dilatation therm. linéique, parallèle 115 E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 115 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 mm -
Inflammabilité pr. épaisseur h HB class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 mm -
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 3.4 - IEC 62631-2-1
Permittivité relative, 1MHz 3.2 - IEC 62631-2-1
Facteur de pertes, 100Hz 19 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 219 E-4 IEC 62631-2-1
Résistivité transversale >1E13 Ohm*m IEC 62631-3-1
Résistivité superficielle 1E13 Ohm IEC 62631-3-2
Rigidité diélectrique 39 kV/mm IEC 60243-1
Indice de résistance au cheminement 600 - IEC 60112
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.4 % Sim. to ISO 62
Absorption d'humidité 0.25 % Sim. to ISO 62
Masse volumique 1300 kg/m³ ISO 1183
Propriétés spécifiques à la matièreValeurUnitéNorme du test
ISO Data
Indice de viscosité 160 cm³/g ISO 307, 1157, 1628
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 80 - 120 °C -
Pré-séchage - temps 4 h -
L'humidité de traitement ≤0.04 % -
Température de la matière fondue 260 - 270 °C -
Température du moule 40 - 80 °C -
Caractéristiques
Transformation
Moulage par injection, Extrusion de films, Extrusion de profilés, Extrusion de plaques, Extrusion (autres)
Conditionnement
Granulés
Disponibilité régionale
Autres informations
Moulages par injection
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 260 - 270 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 40 - 80 °C
injection molding, Mold temperature, recommended: 60 °C
Extrusion (autres)
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
Extrusion, Prepreg, Melt temperature: 250 - 270 °C
Extrusion, Pipes, Melt temperature: 250 - 270 °C
Extrusion, cable sheathing, Melt temperature: 260 - 270 °C
Extrusion de profilés
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
Extrusion, Profiles, Melt temperature: 250 - 270 °C
Extrusion de feuilles
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
Extrusion, Plates, Melt temperature: 250 - 270 °C
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.