Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultraform® N2640 Z4 Q600 - (POM+PUR) - BASF

Material Data Center offers the following functions for Ultraform® N2640 Z4 Q600:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultraform datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.

Abbreviated designation according to ISO 1043-1: POM-HI
Designation according to ISO 29988-POM-K,,M-GNPR,2-1
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 5.5 cm³/10min ISO 1133
Température 190 °C -
Charge 2.16 kg -
Température d'éjection 105 °C -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 1700 MPa ISO 527
Contrainte d'écoulement 44 MPa ISO 527
Déformation au seuil d'écoulement 14 % ISO 527
Déformation nominale à la rupture >50 % ISO 527
Module de fluage en traction, 1h 1350 MPa ISO 899-1
Module de fluage en traction, 1000h 1000 MPa ISO 899-1
Résistance au choc Charpy, +23°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 300 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 13 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 8 kJ/m² ISO 179/1eA
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 167 °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 75 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 140 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 130 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 130 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 mm -
Yellow Card disponible oui - -
Inflammabilité pr. épaisseur h HB class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 mm -
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 4.2 - IEC 62631-2-1
Permittivité relative, 1MHz 4.2 - IEC 62631-2-1
Facteur de pertes, 100Hz 110 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 190 E-4 IEC 62631-2-1
Résistivité transversale 1E11 Ohm*m IEC 62631-3-1
Résistivité superficielle 1E14 Ohm IEC 62631-3-2
Rigidité diélectrique 40 kV/mm IEC 60243-1
Indice de résistance au cheminement 600 - IEC 60112
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.8 % Sim. to ISO 62
Absorption d'humidité 0.25 % Sim. to ISO 62
Masse volumique 1350 kg/m³ ISO 1183
Préparation et conditionnement des éprouvettesValeurUnitéNorme du test
ISO Data
Injection, température de la matière fondue 200 °C ISO 294
Injection, température du moule 80 °C ISO 294
Injection, vitesse d'injection 200 mm/s ISO 294
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Température de la matière fondue 190 - 220 °C -
Température du moule 60 - 80 °C -
Fonctions
Viscosité / Vitesse de cisaillement , Ultraform® N2640 Z4 Q600, (POM+PUR), BASF
Contrainte de cisaillement / Vit. de cisaillement , Ultraform® N2640 Z4 Q600, (POM+PUR), BASF
Module de cisaillement dynamique / Température , Ultraform® N2640 Z4 Q600, (POM+PUR), BASF
Contrainte / Déformation , Ultraform® N2640 Z4 Q600, (POM+PUR), BASF
Module sécant / Déformation , Ultraform® N2640 Z4 Q600, (POM+PUR), BASF
Contrainte / Déformation (isochrone) 23°C, Ultraform® N2640 Z4 Q600, (POM+PUR), BASF
Contrainte / Déformation (isochrone) 40°C, Ultraform® N2640 Z4 Q600, (POM+PUR), BASF
Contrainte / Déformation (isochrone) 80°C, Ultraform® N2640 Z4 Q600, (POM+PUR), BASF
Module de fluage / Temps 80°C, Ultraform® N2640 Z4 Q600, (POM+PUR), BASF
Courbe de fluage 80°C, Ultraform® N2640 Z4 Q600, (POM+PUR), BASF
Volume spécifique (pvT) , Ultraform® N2640 Z4 Q600, (POM+PUR), BASF
Module de traction / Température , Ultraform® N2640 Z4 Q600, (POM+PUR), BASF
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Additifs
Agent de démoulage
Caractéristiques
Copolymère
Disponibilité régionale
Autres informations
Moulages par injection
PROCESSING
injection molding, Melt temperature, range: 190 - 220 °C
injection molding, Melt temperature, recommended: 200 °C
injection molding, Mold temperature, range: 60 - 80 °C
injection molding, Mold temperature, recommended: 80 °C
Résistance Chimique
Acides
Acide acétique (masse en 5%) (23°C)
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com