Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse Z PCTG - Copolyester-Z - BASF

Material Data Center offers the following functions for Ultrafuse Z PCTG:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 67.5 cm³/10min ISO 1133
Température 275 °C -
Charge 5 kg -
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de transition vitreuse, 10°C/min 81 °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 69 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 73 °C ISO 75-1/-2
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1200 kg/m³ ISO 1183
3D DataValeurUnitéNorme du test
Other Standards[S]
Module en traction, flat 1760 MPa ISO 527
Module en traction, upright 1670 MPa ISO 527
Résistance à la traction, flat 37.1 MPa ISO 527
Résistance à la traction, upright 13.6 MPa ISO 527
Déformation à la rupture, flat 3.1 % ISO 527
Déformation à la rupture, upright 0.8 % ISO 527
Module de flexion, flat 1610 MPa ISO 178
Module de flexion, on-edge 1780 MPa ISO 178
Module de flexion, upright 1490 MPa ISO 178
Résistance à la flexion, flat 55.5 MPa ISO 178
Résistance à la flexion, on-edge 70.8 MPa ISO 178
Résistance à la flexion, upright 20.2 MPa ISO 178
Résistance au choc Charpy, +23°C, on-edge 9.5 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C, flat 2.1 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), +23°C, on-edge 2.6 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), +23°C, upright 0.9 kJ/m² ISO 179/1eA
Résistance au choc Izod, +23°C, flat 14.3 kJ/m² ISO 180/1U
Résistance au choc Izod, +23°C, on-edge 24.2 kJ/m² ISO 180/1U
Résistance au choc Izod, +23°C, upright 3.4 kJ/m² ISO 180/1U
Résistance au choc Izod avec entaille, +23°C, on-edge 3.4 kJ/m² ISO 180/1A
Résistivité transversale, flat 40000 Ohm*m IEC 62631-3-1
Résistivité transversale, on-edge 130 Ohm*m IEC 62631-3-1
S: These properties are reported by the producer according standards that are different to our defaults.
Caractéristiques
Transformation
Additive Manufacturing
Conditionnement
Monofilament, Noir
Caractéristiques
Amorphe
Applications
Électrotechnique et électrique
Disponibilité régionale
Amérique du nord, Europe, South and Central America
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com