Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® 4000 GF30 - PEEK-GF30 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® 4000 GF30:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Glass fiber-reinforced (30%) polyether ether ketone

VESTAKEEP® 4000 GF30 is a glass fiber-re­inforced (30%) polyether ether ketone for injection molding.

The semi-crystalline polymer features superior mechanical, thermal, and chemical resistance. Parts made from VESTAKEEP® 4000 GF30 are of low flammability.

VESTAKEEP® 4000 GF30 can be processed on common injection molding machines for thermoplastics.

We recommend a melt temperature of 380°C to 400°C during the injection molding process. The mold temperature should be within a range of 160°C to 200°C, preferably 180°C.

VESTAKEEP® 4000 GF30 is supplied as cylindrical pellets in 25kg boxes with moisture-proof polyethylene liners.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

Pigmentation may affect the values.

For guidance processing of VESTAKEEP® 4000 GF30 please follow the general recommendations in our brochure “VESTAKEEP® PEEK Processing Guidelines“.

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.INDUSTRIAL.VESTAKEEP.COM
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 32 cm³/10min ISO 1133
Température 400 °C -
Charge 21.6 kg -
Retrait au moulage, parallèle 0.3 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.7 % ISO 294-4, 2577
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 11000 MPa ISO 527
Contrainte à la rupture 160 MPa ISO 527
Déformation à la rupture 2 % ISO 527
Résistance au choc Charpy, +23°C 70 kJ/m² ISO 179/1eU
Type de défaillance C - -
Résistance au choc Charpy, -30°C 75 kJ/m² ISO 179/1eU
Type de défaillance C - -
Résistance au choc Charpy (entaillé), +23°C 11 kJ/m² ISO 179/1eA
Type de défaillance C - -
Résistance au choc Charpy (entaillé), -30°C 9 kJ/m² ISO 179/1eA
Type de défaillance C - -
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 340 °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 312 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 335 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 335 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 30 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm V-0 class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 mm -
Aptitude à l'allumage 45 % ISO 4589-1/-2
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 1MHz 3.3 - IEC 62631-2-1
Facteur de pertes, 1MHz 40 E-4 IEC 62631-2-1
Résistivité transversale >1E13 Ohm*m IEC 62631-3-1
Résistivité superficielle 1E15 Ohm IEC 62631-3-2
Indice de résistance au cheminement 200 - IEC 60112
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.4 % Sim. to ISO 62
Masse volumique 1500 kg/m³ ISO 1183
Préparation et conditionnement des éprouvettesValeurUnitéNorme du test
ISO Data
Injection, température de la matière fondue 400 °C ISO 294
Injection, température du moule 180 °C ISO 294
Injection, vitesse d'injection 200 mm/s ISO 294
Injection, pression de maintien 120 MPa ISO 294
Fonctions
Module de traction / Température , VESTAKEEP® 4000 GF30, PEEK-GF30, Evonik
Caractéristiques
Transformation
Moulage par injection, Extrusion (autres)
Conditionnement
Granulés
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com