Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® Care M40 3DF - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® Care M40 3DF:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Filament based on high viscosity, unreinforced polyether ether ketone (PEEK) for 3D printed medical devices

VESTAKEEP® Care M40 3DF is extruded from naturally colored, high viscosity VESTAKEEP® Care M40 G PEEK resin. The material is designed for 3d printing of medical devices with up to 30 days body contact.  


Biocompatibility

Biocompatiblity was tested following ISO10993-1 recommendations for a surface medical device with up to 30 days body contact.
 
The material fulfills the requirements of USP<88> class VI.
 
Tests were performed by independent, certified laboratories.

Biocompatibility tests available for VESTAKEEP® Care M40 3DF:


Delivery and packaging
VESTAKEEP® Care M40 3DF filament has a diameter of 1.75 mm ( /- 0.04 mm*). It is supplied on TROGAMID®-spools with 500g. The spools are packaged in double bags to facilitate transfer into clean areas.

The properties listed are for information only and only apply to the VESTAKEEP® Care M40 G resin used in the manufacture of VESTAKEEP® Care M40 3DF. The performance and the purity of any parts manufactured from VESTAKEEP® Care M40 3DF are highly dependent on any 3D- or additive-printing processes, or any other processing, to which the filament is subjected.
Only density and filament diameter apply to VESTAKEEP® Care M40 3DF directly.

*Diameters are tested by a multi-axis laser gauge. The diameter is the average of these axis.


The values presented are typical or average values, they do not constitute a specification. 
 
FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 11 cm³/10min ISO 1133
Température 380 °C -
Charge 5 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 3500 MPa ISO 527
Résistance à la traction 94 MPa ISO 527
Contrainte d'écoulement 94 MPa ISO 527
Déformation au seuil d'écoulement 5 % ISO 527
Résistance au choc Charpy, +23°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 7 kJ/m² ISO 179/1eA
Type de défaillance C - -
Résistance au choc Charpy (entaillé), -30°C 6 kJ/m² ISO 179/1eA
Type de défaillance C - -
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 335 °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min 152 °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 155 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 205 °C ISO 75-1/-2
Température de ramolliss. Vicat, A 335 °C ISO 306
Température de ramolliss. Vicat, B 305 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 60 E-6/K ISO 11359-1/-2
Inflammabilité pr. épaisseur h V-0 class IEC 60695-11-10
Epaisseur de l'éprouvette 3.2 mm -
ASTM Data
Température de fusion 335 °C ASTM D 3418
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.4 % Sim. to ISO 62
Masse volumique 1300 kg/m³ ISO 1183
Densité 1300 kg/m³ ASTM D 792
Caractéristiques
Transformation
Additive Manufacturing
Conditionnement
Monofilament, Couleurs naturelles
Propriétés spéciales
Stabilisé à la chaleur, Opaque
Caractéristiques
Stabilité thermique
Résistance Chimique
Résistance aux acides, Résistance aux alcalis , Résistance chimique générale, Résistance aux solvants, Résistance aux graisses, Stabilité hydrolytique, Résistance aux huiles, Résistance à oxydation
Certifications
Grade médical, USP Class VI approbation
Applications
Médical
Disponibilité régionale
Europe
Autres informations
Extrusion (autres)
Drying recommendations

We recommend to dry the filament prior to usage to avoid stringing, bubbles, or other defects. 

a) Filament on spool: minimum 12 hours at 80°C to 100°C. 100°C must not be exceeded to avoid distortion of the spool.
b) Filament removed from spool: minimum 4 hours at 130°C to 140°C.
 
The maximum drying temperature of the filament is 140°C. Please also pay attention to the instructions of your drying device.



Spool dimensions

For dimensions of the spool, please see drawing below. All dimensions are given in millimeter (mm).
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.