Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® Care ML17 - PA12 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® Care ML17:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Low viscosity polyamide 12 for medical application

VESTAMID® Care ML17 is resistant to body fluids and toxicologically safe.
 

Typical application areas for filled VESTAMID Care ML grades include  catheters, housing parts, monitoring and imaging devices and durable medical equipment.

Advantages at a glance

- High impact resistance

- Easy processability & colorability

- Low sliding friction

- High toughness

- High abrasion resistance

- Density 1.0 g/cc

- High dimensional stability

- High chemical resistance

- Gamma and EtO sterilizable


Biocompatibility of VESTAMID® Care ML
VESTAMID® Care ML grades were tested on biocompatibility for applications within the body of up to 30 days contact time and comply with USP <88> class VI and ISO 10993 standards.

Biocompatibility tests for VESTAMID® Care:
Standard Description
ASTM F756-08 Hemocompatibility
ISO 10993-5 Cytotoxicity
ISO 10993-10 Sensitization: Maximization test according to Magnusson and Kligman
ISO 10993-10 Irritation: Intracutaneous Reactivity
ISO 10993-11 Acute Systemic Toxicity
USP Class VI Acute Systemic Toxicity Intracutaneous Reactivity Muscle Implantation
Processing of VESTAMID® Care
For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 
 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 21 / * cm³/10min ISO 1133
Température 210 / * °C -
Charge 2.16 / * kg -
Retrait au moulage, parallèle 0.7 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.2 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 1400 / 1120 MPa ISO 527
Contrainte d'écoulement 43 / 41 MPa ISO 527
Déformation au seuil d'écoulement 5 / 13 % ISO 527
Déformation nominale à la rupture >50 / 40 % ISO 527
Résistance au choc Charpy, +23°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N / 50 kJ/m² ISO 179/1eU
Type de défaillance - / C(N) - -
Résistance au choc Charpy (entaillé), +23°C 4.5 / 4.5 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Résistance au choc Charpy (entaillé), -30°C 6 / 5 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Dureté Shore D 75 / * - ISO 7619-1
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 178 / * °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min 45 / * °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 50 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 110 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 140 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 150 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 3.8 / - - IEC 62631-2-1
Permittivité relative, 1MHz 2.9 / - - IEC 62631-2-1
Facteur de pertes, 100Hz 500 / - E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 281 / - E-4 IEC 62631-2-1
Résistivité transversale >1E13 / 2.3E12 Ohm*m IEC 62631-3-1
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 1.5 / * % Sim. to ISO 62
Absorption d'humidité 0.7 / * % Sim. to ISO 62
Masse volumique 1020 / - kg/m³ ISO 1183
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Propriétés spéciales
Modifié choc, Stérilisable, Stérilisation par oxyde d'éthylène (EtO), Stérilisation par rayonnement gamma
Caractéristiques
Grade tribologique
Résistance Chimique
Résistance chimique générale
Certifications
Grade médical, Biocompatibility ISO 10993, USP Class VI approbation
Applications
Médical
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com