Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® DX9303 BK E70288 - PA612-I - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® DX9303 BK E70288:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
High-viscosity, plasticized, heat- and light-stabilized, impact-modified polyamide 612 compound for extrusion

VESTAMID® DX9303 BK E70288 is a PA 612 extrusion compound developed for the production of tubing systems with higher requirements for heat resistance.

The melting point of VESTAMID® DX9303 BK E70288 is about 35°C higher than PA 11 and PA 12 compounds, allows higher peak temperatures in use. Thereby this compound fulfills the increased demands resulting from higher temperatures in the engine compartment.

If it is intended to use VESTAMID® DX9303 BK E70288 for fuel lines, certain preconditions must be observed. The Technical Marketing assists you in finding the suitable VESTAMID® compound.
At temperatures above 100°C tubing of VESTAMID® DX9303 BK E70288 allow a higher pressure load than tubing made of PA 12 compounds with comparable flexibility.

The process temperatures should be in the range of 240-270°C.

The material absorbs only little moisture. Therefore dimensions and properties of parts are nearly unaffected through ambient conditions.


Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 11 / * cm³/10min ISO 1133
Température 275 / * °C -
Charge 5 / * kg -
Retrait au moulage, parallèle 2.7 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.9 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 900 / 680 MPa ISO 527
Contrainte d'écoulement 38 / - MPa ISO 527
Déformation au seuil d'écoulement 30 / - % ISO 527
Déformation nominale à la rupture >50 / - % ISO 527
Résistance au choc Charpy, +23°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 87 / 135 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 11 / 15 kJ/m² ISO 179/1eA
Type de défaillance C / C(P)[C(P)] - -
Dureté Shore D 70 / * - ISO 7619-1
C(P): CAMPUS
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 211 / * °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min 20 / * °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 60 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 142 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 159 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 150 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 120 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 4.7 / - - IEC 62631-2-1
Permittivité relative, 1MHz 2.7 / - - IEC 62631-2-1
Facteur de pertes, 100Hz 1450 / - E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 400 / - E-4 IEC 62631-2-1
Résistivité transversale 2E10 / 5.3E8 Ohm*m IEC 62631-3-1
Rigidité diélectrique 39 / 34 kV/mm IEC 60243-1
Indice de résistance au cheminement 600 / - - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 2.4 / * % Sim. to ISO 62
Absorption d'humidité 1 / * % Sim. to ISO 62
Masse volumique 1050 / - kg/m³ ISO 1183
Caractéristiques
Transformation
Extrusion de tubes, Extrusion (autres)
Conditionnement
Granulés, Noir
Additifs
Plastifiant
Propriétés spéciales
Modifié choc, Stabilisé à la lumière, Stabilisé à la chaleur
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com