Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® E62-S3 - TPA - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® E62-S3:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

Heat- and light-stabilized compound based on polyamide 12 elastomer for molding of sport shoe soles

VESTAMID® E62-S3 is a PA 12 elastomer consisting of PA 12 segments and softening segments. The material is free of volatile or migrating plasticizer.

The VESTAMID® E represent thermoplastic elastomers generically characterized as polyether block copolyamides (PEBA) consisting of PA 12 and polyether segments.
 
VESTAMID® E62-S3 is especially developed for sport shoe soles. It has good impact strength at low temperatures.

VESTAMID® E62-S3 is supplied as spherical pellets in moisture-proof packaging, ready for processing.
 
The process temperatures should be within a range of 190°C – 230°C.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 20 / * cm³/10min ISO 1133
Température 240 / * °C -
Charge 2.16 / * kg -
Retrait au moulage, parallèle 0.8 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.4 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 370 / 365 MPa ISO 527
Contrainte d'écoulement 23 / 24 MPa ISO 527
Déformation au seuil d'écoulement 30 / 26 % ISO 527
Déformation nominale à la rupture >50 / >50 % ISO 527
Résistance au choc Charpy, +23°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 120 / 112 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 8 / 11 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Résistance au choc en traction, +23°C 230 / - kJ/m² ISO 8256/1
Contrainte à 10% de déformation 19 / * MPa ISO 527
Contrainte à 100% de déformation 23 / * MPa ISO 527
Contrainte à 300% de déformation 40 / * MPa ISO 527
Déformation à la rupture TPE >300 / * % ISO 527
Déformation rémanente en compression à 23 °C, 24h 34 / * % ISO 815
Déformation rémanente en compression à 70 °C, 24h 48 / * % ISO 815
Déformation rémanente en compression à 100 °C, 24h 85 / * % ISO 815
Dureté Shore D 62 / * - ISO 7619-1
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 172 / * °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min 10 / * °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 45 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 100 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 110 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 200 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 200 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 9 / - - IEC 62631-2-1
Permittivité relative, 1MHz 4 / - - IEC 62631-2-1
Facteur de pertes, 100Hz 1000 / - E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 1200 / - E-4 IEC 62631-2-1
Résistivité transversale 2E10 / 2.5E9 Ohm*m IEC 62631-3-1
Rigidité diélectrique 39 / 35 kV/mm IEC 60243-1
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 1.1 / * % Sim. to ISO 62
Absorption d'humidité 0.5 / * % Sim. to ISO 62
Masse volumique 1030 / - kg/m³ ISO 1183
Fonctions
Viscosité / Vitesse de cisaillement , VESTAMID® E62-S3, TPA, Evonik
Contrainte de cisaillement / Vit. de cisaillement , VESTAMID® E62-S3, TPA, Evonik
Contrainte / Déformation , VESTAMID® E62-S3 (sec), TPA, Evonik
Module sécant / Déformation , VESTAMID® E62-S3 (sec), TPA, Evonik
Contrainte / Déformation (TPE) , VESTAMID® E62-S3, TPA, Evonik
Contrainte / Déformation (isochrone) 23°C, VESTAMID® E62-S3 (cond.), TPA, Evonik
Module de fluage / Temps 23°C, VESTAMID® E62-S3 (cond.), TPA, Evonik
Courbe de fluage 23°C, VESTAMID® E62-S3 (cond.), TPA, Evonik
Volume spécifique (pvT) , VESTAMID® E62-S3, TPA, Evonik
Module de traction / Température , VESTAMID® E62-S3 (sec), TPA, Evonik
Caractéristiques
Transformation
Moulage par injection, Extrusion de profilés, Extrusion (autres)
Conditionnement
Granulés
Propriétés spéciales
Stabilisé à la lumière, Stabilisé aux intempéries, Stabilisé à la chaleur
Applications
Sport
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.