Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® L-GF15 - PA12-GF15 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® L-GF15:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

Glass fibre reinforced (15%) PA12 resin for the injection moulding of rigid and tough parts


VESTAMID® L-GF15 NC is a glass fiber –reinforced heat stabilized Polyamide 12 for injection molding. The material contains about 15% glass fibers, an ageing protective agent and a processing aid for a fast and even form filling. Due to the reinforcement moldings from this compound exhibit a higher strength and good heat resistance, excellent for gear housings for electric window openers in cars.


Further advantages of VESTAMID® L-GF15 NC are the characterizing properties of PA12, e.g., low water absorption, good dimensional stability and nearly constant mechanical properties at changing ambient humidity.

  
VESTAMID® L-GF15 NC is supplied as cylindrical granules, ready for processing, in moisture-proof bags.

 
The use of colorants may change property values.


Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.


For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 
 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM

OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 55 / * cm³/10min ISO 1133
Température 275 / * °C -
Charge 5 / * kg -
Retrait au moulage, parallèle 0.3 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.7 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 4200 / 3600 MPa ISO 527
Contrainte d'écoulement 90 / 81 MPa ISO 527
Déformation au seuil d'écoulement 4 / 4 % ISO 527
Déformation nominale à la rupture 5 / 4 % ISO 527
Résistance au choc Charpy, +23°C 64 / 49 kJ/m² ISO 179/1eU
Type de défaillance C / C - -
Résistance au choc Charpy, -30°C 80 / 55 kJ/m² ISO 179/1eU
Type de défaillance C / C - -
Résistance au choc Charpy (entaillé), +23°C 12 / 9 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Résistance au choc Charpy (entaillé), -30°C 11 / 7 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 178 / * °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 160 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 175 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 170 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 80 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Yellow Card disponible oui / * - -
Yellow Card disponible oui / * - -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 4 / 5.2 - IEC 62631-2-1
Permittivité relative, 1MHz 3.4 / 3.3 - IEC 62631-2-1
Facteur de pertes, 100Hz 380 / - E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 260 / 450 E-4 IEC 62631-2-1
Résistivité transversale >1E13 / 1.8E12 Ohm*m IEC 62631-3-1
Rigidité diélectrique 50 / 47 kV/mm IEC 60243-1
Indice de résistance au cheminement 600 / - - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 1.3 / * % Sim. to ISO 62
Absorption d'humidité 0.6 / * % Sim. to ISO 62
Masse volumique 1120 / - kg/m³ ISO 1183
Préparation et conditionnement des éprouvettesValeurUnitéNorme du test
ISO Data
Injection, température de la matière fondue 260 °C ISO 294
Injection, température du moule 80 °C ISO 294
Injection, vitesse d'injection 200 mm/s ISO 294
Injection, pression de maintien 70 MPa ISO 294
Fonctions
Viscosité / Vitesse de cisaillement , VESTAMID® L-GF15, PA12-GF15, Evonik
Contrainte de cisaillement / Vit. de cisaillement , VESTAMID® L-GF15, PA12-GF15, Evonik
Module de cisaillement dynamique / Température , VESTAMID® L-GF15 (sec), PA12-GF15, Evonik
Contrainte / Déformation , VESTAMID® L-GF15 (sec), PA12-GF15, Evonik
Module sécant / Déformation , VESTAMID® L-GF15 (sec), PA12-GF15, Evonik
Contrainte / Déformation (isochrone) 23°C, VESTAMID® L-GF15 (cond.), PA12-GF15, Evonik
Module de fluage / Temps 23°C, VESTAMID® L-GF15 (cond.), PA12-GF15, Evonik
Courbe de fluage 23°C, VESTAMID® L-GF15 (cond.), PA12-GF15, Evonik
Module de traction / Température , VESTAMID® L-GF15 (sec), PA12-GF15, Evonik
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés, Couleurs naturelles
Additifs
Lubrifiant
Propriétés spéciales
Stabilisé à la chaleur
Applications
Automobile
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com