Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® L-GF50 BK 9.7506 - PA12-GF50 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® L-GF50 BK 9.7506:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Medium-viscosity, heat-stabilized glass fiber-reinforced polyamide 12  compound

VESTAMID® L-GF50 BK 9.7506 is a 50% glass fiber-reinforced, easily demoldable and heat-stabilized polyamide 12 compound.

Due to its mold release properties, VESTAMID® L-GF50 BK 9.7506 is suitable for the efficient production of injection molded parts with short cycle times.

Further advantages of VESTAMID® L-GF50 BK 9.7506 are the characteristic properties of polyamide 12 as low water absorption, good dimensional stability and almost the same properties at changing ambient humidity.
  
VESTAMID® L-GF50 BK 9.7506 is supplied as cylindrical granules, ready for processing, in moisture-proof bags.
   
Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 9 / * cm³/10min ISO 1133
Température 275 / * °C -
Charge 2.16 / * kg -
Retrait au moulage, parallèle 0.2 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.7 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 12000 / - MPa ISO 527
Contrainte d'écoulement 150 / - MPa ISO 527
Déformation au seuil d'écoulement 4 / - % ISO 527
Déformation nominale à la rupture 4.5 / - % ISO 527
Résistance au choc Charpy, +23°C 90 / - kJ/m² ISO 179/1eU
Type de défaillance C / - - -
Résistance au choc Charpy, -30°C 90 / - kJ/m² ISO 179/1eU
Type de défaillance C / - - -
Résistance au choc Charpy (entaillé), +23°C 25 / - kJ/m² ISO 179/1eA
Type de défaillance C / - - -
Résistance au choc Charpy (entaillé), -30°C 17 / - kJ/m² ISO 179/1eA
Type de défaillance C / - - -
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 177 / * °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min 41 / * °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 172 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 179 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 175 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 14 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 131 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Inflammabilité pr. épaisseur h HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 / * mm -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 4.9 / - - IEC 62631-2-1
Permittivité relative, 1MHz 3.8 / - - IEC 62631-2-1
Facteur de pertes, 100Hz 510 / - E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 320 / - E-4 IEC 62631-2-1
Résistivité transversale 1E12 / - Ohm*m IEC 62631-3-1
Rigidité diélectrique 33 / - kV/mm IEC 60243-1
Indice de résistance au cheminement 600 / - - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 0.83 / * % Sim. to ISO 62
Absorption d'humidité 0.44 / * % Sim. to ISO 62
Masse volumique 1450 / - kg/m³ ISO 1183
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés, Noir
Additifs
Agent de démoulage
Propriétés spéciales
Stabilisé à la chaleur
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.