Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® LX9013 BK 9.7507 - PA12-I - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® LX9013 BK 9.7507:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

High-viscosity, plasticized compound for extrusion with an extraordinary long-term heat resistance

VESTAMID® LX9013 BK 9.7507 is a plasticized polyamide 12 compound with an especially high long-term resistance under thermal load.

The material absorbs only little moisture, thus leading to nearly unaffected dimensions and properties of the finished parts at changing ambient conditions. Extruded tubes are impact-resistant also at low temperatures.

VESTAMID® LX9013 BK 9.7507 is suited to produce flexible tubes that are permanently exposed to higher temperatures, e.g., in the engine compartment of motor vehicles. Especially when used as diesel fuel lines they show significant advantages compared with standard grades, obvious in storage tests with diesel fuel (see the figure).

The material corresponds to the extrusion compound PA12-HIPHL, grade1 acc. DIN 73378 and meets the requirements acc. DIN 74324 (black), ISO 7628 and SAE J844.

VESTAMID® LX9013 BK 9.7507 is supplied as pellets in moisture-proof packaging ready for processing.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Retrait au moulage, parallèle 0.4 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.5 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 410 / 400 MPa ISO 527
Résistance au choc Charpy, +23°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 130 / 140 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 7 / 20 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Dureté Shore D 65 / * - ISO 7619-1
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 172 / * °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min 0 / * °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 55 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 130 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 130 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 160 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 160 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 12 / 15.6 - IEC 62631-2-1
Permittivité relative, 1MHz 3.4 / 3.6 - IEC 62631-2-1
Facteur de pertes, 100Hz 5000 / 6650 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 1000 / 1390 E-4 IEC 62631-2-1
Résistivité transversale 1E8 / 5.1E7 Ohm*m IEC 62631-3-1
Rigidité diélectrique 25 / 23 kV/mm IEC 60243-1
Indice de résistance au cheminement 600 / - - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 1.5 / * % Sim. to ISO 62
Absorption d'humidité 0.6 / * % Sim. to ISO 62
Masse volumique 1020 / 1020 kg/m³ ISO 1183
Caractéristiques
Transformation
Extrusion de tubes, Extrusion de profilés, Extrusion (autres)
Conditionnement
Granulés, Noir
Additifs
Plastifiant
Propriétés spéciales
Modifié choc, Stabilisé à la chaleur
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.