Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® Care ME71 - TPA - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® Care ME71:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Polyamide 12 elastomer molding compounds

VESTAMID® Care ME71 is free of plasticizers and heat and light stabilized. VESTAMID® Care ME71 is resistant to body fluids and toxicologically safe.

VESTAMID® Care ME grades are flexible polyether block amides (PEBA) resins.

The advantages at a glance:
  • High flexibility & elasticity
  • Good rebound properties
  • High impact resistance
  • Excellent dimensional stability
  • High chemical resistance
  • Easy processability & colorability
  • Plasticizer-free
  • Gamma and EtO sterilization resistant
  • Tough and resilient

Biocompatibility of VESTAMID® Care ME

Biocompatiblity was tested following ISO10993-1 recommendations for a surface medical device with up to 30 days body contact.
 
The material fulfills the requirements of USP<88> class VI.
 
Tests were performed by independent, certified laboratories.

Biocompatibility tests for VESTAMID® Care:
Standard Description
ASTM F756-08 Hemocompatibility
ISO 10993-5 Cytotoxicity
ISO 10993-10 Sensitization: Maximization test according to Magnusson and Kligman
ISO 10993-10 Irritation: Intracutaneous Reactivity
ISO 10993-11 Acute Systemic Toxicity
USP Class VI Acute Systemic Toxicity Intracutaneous Reactivity Muscle Implantation


Processing of VESTAMID® Care
For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 75 / * cm³/10min ISO 1133
Température 240 / * °C -
Charge 2.16 / * kg -
Retrait au moulage, parallèle 1.2 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.3 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 1090 / 760 MPa ISO 527
Contrainte d'écoulement 39 / 34 MPa ISO 527
Déformation au seuil d'écoulement 13 / 16 % ISO 527
Déformation nominale à la rupture >50 / >50 % ISO 527
Résistance au choc Charpy, +23°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 5 / 7 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Résistance au choc Charpy (entaillé), -30°C 6 / 4 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Dureté Shore D 71 / * - ISO 7619-1
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 177 / * °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 54 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 111 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 137 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 150 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 155 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 4.5 / - - IEC 62631-2-1
Permittivité relative, 1MHz 3.2 / - - IEC 62631-2-1
Facteur de pertes, 100Hz 760 / - E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 334 / - E-4 IEC 62631-2-1
Résistivité transversale 4E12 / 2.9E11 Ohm*m IEC 62631-3-1
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 1.5 / * % Sim. to ISO 62
Absorption d'humidité 0.7 / * % Sim. to ISO 62
Masse volumique 1010 / - kg/m³ ISO 1183
Préparation et conditionnement des éprouvettesValeurUnitéNorme du test
ISO Data
Injection, température de la matière fondue 220 °C ISO 294
Injection, température du moule 35 °C ISO 294
Injection, vitesse d'injection 200 mm/s ISO 294
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Propriétés spéciales
Modifié choc, Stabilisé à la lumière, Stabilisé à la chaleur, Stérilisable, Stérilisation par oxyde d'éthylène (EtO), Stérilisation par rayonnement gamma
Résistance Chimique
Résistance chimique générale
Certifications
Grade médical, Biocompatibility ISO 10993, USP Class VI approbation
Applications
Médical
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.