Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® EX9350 BK E70293 - TPA-I - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® EX9350 BK E70293:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

Heat- and weather-resistant, impact-modified polyamide 612 elastomer for extrusion

VESTAMID® EX9350 BK E70293 is a PA 612 elastomer extrusion compound developed for the manufacturing of tubing systems, e.g. vacuum brake booster lines.

The compound is in particular suitable for applications, that require a continuous high flexibility even if subjected to high temperature load. In contrast to conventionally plasticized materials (plasticizerloss) tubes made from VESTAMID® EX9350 BK E70293 do not stiffen under elevated temperatures.

In comparison with PA 11 and PA 12 compounds the increased melting point allows for increased peak temperatures in use.

The compound is especially suitable for the extrusion of tubing systems that are exposed to increased burst pressures and service temperatures.

The process temperatures should be within a range of 210 to 240 °C.

VESTAMID® EX9350 BK E70293 is supplied as cylindrical pellets in moisture-proof packaging, ready for use.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 
 

The values presented are typical or average values, they do not constitute a specification.
 
FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 56 / * cm³/10min ISO 1133
Température 280 / * °C -
Charge 2.16 / * kg -
Retrait au moulage, parallèle 1.1 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.0 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 630 / 480 MPa ISO 527
Contrainte d'écoulement 30 / 26 MPa ISO 527
Déformation au seuil d'écoulement 30 / 31 % ISO 527
Déformation nominale à la rupture >50 / >50 % ISO 527
Résistance au choc Charpy, +23°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 30 / 130 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 8 / 6 kJ/m² ISO 179/1eA
Type de défaillance C / C - -
Dureté Shore D 67 / * - ISO 7619-1
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 198 / * °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min -4 / * °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 50 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 130 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 130 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 122 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 140 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 8.3 / - - IEC 62631-2-1
Permittivité relative, 1MHz 3.4 / - - IEC 62631-2-1
Facteur de pertes, 100Hz 2940 / - E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 616 / - E-4 IEC 62631-2-1
Résistivité transversale 8.6E8 / 6E7 Ohm*m IEC 62631-3-1
Rigidité diélectrique 35 / 26 kV/mm IEC 60243-1
Indice de résistance au cheminement 575 / - - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 1.1 / * % Sim. to ISO 62
Absorption d'humidité 3.5 / * % Sim. to ISO 62
Masse volumique 1050 / - kg/m³ ISO 1183
Préparation et conditionnement des éprouvettesValeurUnitéNorme du test
ISO Data
Injection, température de la matière fondue 250 °C ISO 294
Injection, température du moule 80 °C ISO 294
Injection, vitesse d'injection 200 mm/s ISO 294
Caractéristiques
Transformation
Extrusion de tubes, Extrusion de profilés, Extrusion (autres)
Conditionnement
Granulés, Noir
Propriétés spéciales
Modifié choc, Stabilisé à la lumière, Stabilisé aux intempéries, Stabilisé à la chaleur
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.