Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® LX9042 NC - PA12 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® LX9042 NC:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Heat stabilized polyamide 12 compound

VESTAMID® LX9042 NC 
is an easy mold release and heat stabilized compound. Due to its highly effective mold release agents, VESTAMID® LX9042 NC is suitable for the efficient production of injection molded parts with very short cycle times.

In addition, VESTAMID® LX9042 NC is nucleated to reduce the cycle time even further and/or to reduce the shrinkage.

Properties of compounds based on Polyamide12 vary little with changing humidity due to their low moisture absorption.

Parts made of this semicrystalline material are characterized by exceptional impact strength, low coefficient of friction and good chemical resistance.
 
VESTAMID® LX9042 NC is supplied as cylindrical granules, ready for processing, in moisture-proof bags.

Pigmentation may affect values.

The results shown have been generated from a low number of production lots. Therefore, they are preliminary and not yet the result of a statistical evaluation. Therefore they must not be used to establish specifications.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 9 / * cm³/10min ISO 1133
Température 220 / * °C -
Charge 2.16 / * kg -
Retrait au moulage, parallèle 0.7 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.7 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 1600 / - MPa ISO 527
Contrainte d'écoulement 47 / - MPa ISO 527
Déformation au seuil d'écoulement 11 / - % ISO 527
Déformation nominale à la rupture >50 / - % ISO 527
Résistance au choc Charpy, +23°C N / - kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 4.6 / - kJ/m² ISO 179/1eA
Type de défaillance C / - - -
Résistance au choc Charpy (entaillé), -30°C 4.6 / - kJ/m² ISO 179/1eA
Type de défaillance C / - - -
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 180 / * °C ISO 11357-1/-3
Température de ramolliss. Vicat, B 154 / * °C ISO 306
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 0.04 / * % Sim. to ISO 62
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés, Couleurs naturelles
Additifs
Agent de démoulage
Propriétés spéciales
Modifié choc, Stabilisé à la chaleur
Caractéristiques
Nuclée, Grade tribologique
Résistance Chimique
Résistance chimique générale
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.