Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTODUR® GF30-FR3 NC - PBT-GF30 FR(17) - Evonik Operations GmbH

Material Data Center offers the following functions for VESTODUR® GF30-FR3 NC:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Vestodur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

Glass Fiber Reinforced and Flame Retardant Polybutylene Terephthalate Compound

VESTODUR® GF30-FR3 is a glass fiber-reinforced (30% glass fiber), semi-crystalline thermoplastic compound for injection molding, based on polybutylene terephthalate (PBT), with a creamy-white color.
 
Test bars made of this compound are rated V-0, according UL94 by Underwriters Laboratories Inc., self-extinguishing and non-dripping.
 
This compound is especially suitable for parts which are subjected to high mechanical and thermal loads and must have a very good flame-resistance.

The incorporated flame retardant is non-migrating and does not contain polybrominated diphenyl ethers. The additive has no corrosive effects on metal inserts or neighboring metal parts.

Therefore, the compound is suitable for components of the electrical and electronical industry. Laser marking with high contrasts is possible.
 
The compounds are supplied as cylindrical pellets in polyethylene packaging.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.


FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM 
OR VISIT OUR PRODUCT AT WWW.VESTODUR.COM

Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 12 cm³/10min ISO 1133
Température 250 °C -
Charge 2.16 kg -
Retrait au moulage, parallèle 0.2 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.5 % ISO 294-4, 2577
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 11400 MPa ISO 527
Contrainte à la rupture 130 MPa ISO 527
Déformation à la rupture 2.2 % ISO 527
Module de fluage en traction, 1h 11000 MPa ISO 899-1
Module de fluage en traction, 1000h 8000 MPa ISO 899-1
Résistance au choc Charpy, +23°C 55 kJ/m² ISO 179/1eU
Type de défaillance C - -
Résistance au choc Charpy (entaillé), +23°C 9 kJ/m² ISO 179/1eA
Type de défaillance C - -
Dureté Shore D 84 - ISO 7619-1
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 223 °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min 45 °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 216 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 223 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 213 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 50 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm V-0 class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 mm -
Inflammabilité pr. épaisseur h V-0 class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 mm -
Aptitude à l'allumage 34 % ISO 4589-1/-2
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 4.1 - IEC 62631-2-1
Permittivité relative, 1MHz 4.4 - IEC 62631-2-1
Facteur de pertes, 100Hz 30 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 150 E-4 IEC 62631-2-1
Résistivité transversale >1E13 Ohm*m IEC 62631-3-1
Résistivité superficielle 1E13 Ohm IEC 62631-3-2
Indice de résistance au cheminement 250 - IEC 60112
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.4 % Sim. to ISO 62
Masse volumique 1720 kg/m³ ISO 1183
Fonctions
Module de cisaillement dynamique / Température , VESTODUR® GF30-FR3 NC, PBT-GF30 FR(17), Evonik
Volume spécifique (pvT) , VESTODUR® GF30-FR3 NC, PBT-GF30 FR(17), Evonik
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés, Couleurs naturelles, Blanc
Additifs
Agent de démoulage, Agent ignifugeant
Propriétés spéciales
Ignifugé, Stabilisé à la lumière, Stabilisé aux intempéries, Stabilisé à la chaleur
Caractéristiques
Marquage au laser
Applications
Électrotechnique et électrique
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.