Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTODUR® X4877 NC - PBT-I-GF30 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTODUR® X4877 NC:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Vestodur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

Easy-flow, glass fiber-reinforced polybutylene terephthalate compound with increased impact strength

VESTODUR® X4877 is an easy-flow, glass  fiber-reinforced (30%) polybutylene tereph­thalate compound (PBT) with increased impact strength for injection molding.

 

This compound is especially suitable for the manufacture of parts which are subjected to  high mechanical and thermal loads. Compared with commonly used glass fiber-reinforced

PBT compounds with a similar stiffness VESTODUR® X4877 has an increased impact strength and also a higher strain at break.

 

VESTODUR® X4877 is supplied as cylindrical pellets in polyethylene packaging.

 

For further information about processing of VESTODUR® X4877, please follow the general recommendations in our brochure "VESTODUR® Handling and Processing".

 

Pigmentation may affect values.
 

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.


FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM 
OR VISIT OUR PRODUCT AT WWW.VESTODUR.COM

Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 20 / * cm³/10min ISO 1133
Température 250 / * °C -
Charge 2.16 / * kg -
Retrait au moulage, parallèle 0.3 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.0 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 5200 / - MPa ISO 527
Contrainte à la rupture 100 / - MPa ISO 527
Déformation à la rupture 5.5 / - % ISO 527
Module de fluage en traction, 1h * / 5200 MPa ISO 899-1
Module de fluage en traction, 1000h * / 4500 MPa ISO 899-1
Résistance au choc Charpy, +23°C 80 / - kJ/m² ISO 179/1eU
Type de défaillance C / - - -
Résistance au choc Charpy (entaillé), +23°C 16 / - kJ/m² ISO 179/1eA
Type de défaillance C / - - -
Résistance au choc Charpy (entaillé), -30°C 13 / - kJ/m² ISO 179/1eA
Type de défaillance C / - - -
Dureté Shore D 79 / * - ISO 7619-1
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 200 / * °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 175 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 195 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 165 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 50 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Inflammabilité pr. épaisseur h HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 / * mm -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 4.7 / - - IEC 62631-2-1
Facteur de pertes, 100Hz 200 / - E-4 IEC 62631-2-1
Résistivité transversale 1E12 / - Ohm*m IEC 62631-3-1
Résistivité superficielle * / 1E13 Ohm IEC 62631-3-2
Indice de résistance au cheminement 600 / - - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 0.25 / * % Sim. to ISO 62
Masse volumique 1490 / - kg/m³ ISO 1183
Fonctions
Module de cisaillement dynamique / Température , VESTODUR® X4877 NC (sec), PBT-I-GF30, Evonik
Volume spécifique (pvT) , VESTODUR® X4877 NC, PBT-I-GF30, Evonik
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés, Couleurs naturelles
Additifs
Lubrifiant, Agent de démoulage
Propriétés spéciales
Modifié choc, Stabilisé à la chaleur
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.