Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Victrex HT - PEK - Victrex plc

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Victrex HT" in Material Data Center leads to the following information:

Tradename: Victrex HT
Family: PEK
Producer: Victrex plc
8 hits in the material database
2 hits in the literature database
2 hits in the application database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
VICTREX® HT™ 22CA30 PEK-CF30
VICTREX® HT™ 22GL30 PEK-GF30
VICTREX® HT™ G22 PEK
VICTREX® HT™ G45 PEK
VICTREX® HT™ P22 PEK
VICTREX® HT™ P22PF PEK
VICTREX® HT™ P45 PEK
VICTREX® HT™ P45PF PEK

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.