Caractéristiques des transformations/physiques | Valeur | Unité | Norme du test |
ASTM Data |
Indice de fluidité, MFI |
3.7 |
g/10min |
ASTM D 1238 |
Température |
190 |
°C |
- |
Charge |
2.16 |
kg |
- |
Propriétés thermiques | Valeur | Unité | Norme du test |
Other Standards[S] |
Température de fusion |
106 |
°C |
ExxonMobil Method |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés optiques | Valeur | Unité | Norme du test |
ASTM Data |
Brillant |
89 |
- |
ASTM D 2457 |
Other Standards[S] |
Haze |
0.4 |
% |
ExxonMobil Method |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés diverses | Valeur | Unité | Norme du test |
Other Standards[S] |
Densité |
889 |
kg/m³ |
ExxonMobil Method |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés mécaniques (Grades film) | Valeur | Unité | Norme du test |
ASTM Data |
Type d'extrusion |
cast |
- |
- |
Epaisseur des eprouvettes |
0.0254 |
mm |
- |
Other Standards[S] |
Module de traction d’élasticité, long. |
15.2 |
MPa |
ExxonMobil Method |
Module de traction d’élasticité, trav. |
13.1 |
MPa |
ExxonMobil Method |
Résistance de traction à la rupture, long. |
62.7 |
MPa |
ExxonMobil Method |
Résistance de traction à la rupture, trav. |
35.9 |
MPa |
ExxonMobil Method |
Allongement à la rupture, long. |
440 |
% |
ExxonMobil Method |
Allongement à la rupture, trav. |
790 |
% |
ExxonMobil Method |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Caractéristiques
Transformation
Extrusion de films
Caractéristiques
Copolymère
Certifications
RoHS
Applications
Emballage
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com