Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vydyne® R525H BK0201 - PA66-GF25 - Ascend

Material Data Center offers the following functions for Vydyne® R525H BK0201:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vydyne datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Vydyne R525H BK0201 is a general purpose, 25% glass-filled, heat-stabilized, high viscosity PA66 based resin designed for injection molding applications. R525H BK0201 offers standard flow with a black surface finish and maintains the excellent resistance typical of PA66 in chemicals, machine and motor oils, solvents, and gasoline.
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Retrait au moulage, parallèle 0.5 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.3 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 8600 / 5500 MPa ISO 527
Contrainte à la rupture 174 / 117 MPa ISO 527
Déformation à la rupture 3 / 7 % ISO 527
Module de flexion, 23°C 7700 / 5700 MPa ISO 178
Résistance à la flexion 250 / 150 MPa ISO 178
Résistance au choc Charpy, +23°C 59 / 69 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 56 / 56 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 9 / 9 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 8 / 8 kJ/m² ISO 179/1eA
Résistance au choc Izod avec entaille, +23°C 10 / 15 kJ/m² ISO 180/1A
Résistance au choc Izod avec entaille 9 / 10 kJ/m² ISO 180/1A
Température -30 °C -
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 262 / * °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 244 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 259 / * °C ISO 75-1/-2
Coeffic. de dilatation therm. linéique, parallèle 26 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 76 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 / * mm -
Inflammabilité pr. épaisseur h HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 / * mm -
Glow Wire Flammability Index (GWFI) 675 °C IEC 60695-2-12
GWFI - thickness tested (1) 0.75 mm -
Glow Wire Flammability Index (GWFI) 675 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.5 mm -
Glow Wire Flammability Index (GWFI) 675 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 700 °C IEC 60695-2-13
GWIT - thickness tested (1) 0.75 mm -
Glow Wire Ignition Temperature (GWIT) 700 °C IEC 60695-2-13
GWIT - thickness tested (2) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 700 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
UL 94 inflammabilité HB - UL 94
Épaisseur testée 0.75 mm -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Résistivité transversale 1E11 / - Ohm*m IEC 62631-3-1
Rigidité diélectrique 20 / - kV/mm IEC 60243-1
Indice de résistance au cheminement 325 / - - IEC 60112
ASTM Data
Résistance à l’arc 90 / - s ASTM D 495
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 1.4 / * % Sim. to ISO 62
Absorption d'humidité 1.9 / * % Sim. to ISO 62
Masse volumique 1320 / - kg/m³ ISO 1183
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 80 °C -
Pré-séchage - temps 4 h -
Température de la matière fondue 285 - 305 °C -
Température du moule 65 - 95 °C -
Zone 1 280 - 310 °C -
Zone 2 280 - 310 °C -
Zone 3 280 - 310 °C -
Température de la buse 280 - 310 °C -
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés, Noir
Additifs
Lubrifiant
Propriétés spéciales
Stabilisé à la chaleur
Caractéristiques
Résistance à la fatigue
Résistance Chimique
Résistance chimique générale, Résistance aux solvants, Stabilité hydrolytique, Résistance aux huiles
Applications
Automobile, General Purpose
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.