Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vydyne® R513H NT - PA66-GF13 - Ascend

Material Data Center offers the following functions for Vydyne® R513H NT:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vydyne datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Vydyne R513H NT is a general purpose, 13% glass-filled, heat-stabilized PA66 based resin designed for injection molding applications. R513H BK02 offers improved flow with a natural surface finish and maintains the excellent resistance typical of PA66 in chemicals, machine and motor oils, solvents, and gasoline.
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Retrait au moulage, parallèle 0.5 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.0 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 6200 / 3900 MPa ISO 527
Contrainte à la rupture 115 / 75 MPa ISO 527
Déformation à la rupture 3 / 13 % ISO 527
Module de flexion, 23°C 5200 / 3150 MPa ISO 178
Résistance à la flexion 165 / 106 MPa ISO 178
Résistance au choc Charpy, +23°C 38 / 42 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 31 / 37 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 6 / 7.5 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 6 / 5.3 kJ/m² ISO 179/1eA
Résistance au choc Izod avec entaille, +23°C 5.1 / 8.5 kJ/m² ISO 180/1A
Résistance au choc Izod avec entaille 5 / 5.4 kJ/m² ISO 180/1A
Température -30 °C -
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 260 / * °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 240 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 258 / * °C ISO 75-1/-2
Coeffic. de dilatation therm. linéique, parallèle 30 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 113 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 / * mm -
Inflammabilité pr. épaisseur h HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 / * mm -
Aptitude à l'allumage 25 / * % ISO 4589-1/-2
Glow Wire Flammability Index (GWFI) 675 °C IEC 60695-2-12
GWFI - thickness tested (1) 0.75 mm -
Glow Wire Flammability Index (GWFI) 675 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.5 mm -
Glow Wire Flammability Index (GWFI) 675 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 700 °C IEC 60695-2-13
GWIT - thickness tested (1) 0.75 mm -
Glow Wire Ignition Temperature (GWIT) 700 °C IEC 60695-2-13
GWIT - thickness tested (2) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 700 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
UL 94 inflammabilité HB - UL 94
Épaisseur testée 0.75 mm -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Résistivité transversale 1E11 / - Ohm*m IEC 62631-3-1
Rigidité diélectrique 20 / - kV/mm IEC 60243-1
Indice de résistance au cheminement 325 / - - IEC 60112
ASTM Data
Résistance à l’arc 90 / - s ASTM D 495
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 1 / * % Sim. to ISO 62
Absorption d'humidité 2.2 / * % Sim. to ISO 62
Masse volumique 1230 / - kg/m³ ISO 1183
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 80 °C -
Pré-séchage - temps 4 h -
Température de la matière fondue 285 - 305 °C -
Température du moule 65 - 95 °C -
Zone 1 280 - 310 °C -
Zone 2 280 - 310 °C -
Zone 3 280 - 310 °C -
Température de la buse 280 - 310 °C -
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés, Couleurs naturelles
Additifs
Lubrifiant, Agent de démoulage
Propriétés spéciales
Modifié choc, Stabilisé à la chaleur
Caractéristiques
Résistance au fluage
Résistance Chimique
Résistance chimique générale, Résistance aux solvants, Résistance aux graisses, Résistance aux huiles
Certifications
Contact alimentaire, Approuvé pour le contact alimentaire suivant 10/2011, FDA 21 CFR approbation
Applications
Automobile, General Purpose
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.