Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Xyron™ X551V - PPE-X10 - Asahi Kasei

Material Data Center offers the following functions for Xyron™ X551V:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Xyron datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Résistance à la traction 54 MPa ISO 527
Module de flexion, 23°C 3900 MPa ISO 178
Résistance à la flexion 110 MPa ISO 178
Résistance au choc Charpy (entaillé), +23°C 4 kJ/m² ISO 179/1eA
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 118 °C ISO 75-1/-2
Coeffic. de dilatation therm. linéique, parallèle 60 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm V-1 class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 mm -
ASTM Data
DTUL à 264 psi 120 °C ASTM D 648
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 3.1 - IEC 62631-2-1
Permittivité relative, 1MHz 3 - IEC 62631-2-1
Facteur de pertes, 100Hz 30 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 50 E-4 IEC 62631-2-1
Résistivité transversale 1E14 Ohm*m IEC 62631-3-1
Résistivité superficielle 1E16 Ohm IEC 62631-3-2
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1150 kg/m³ ISO 1183
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 100 - 110 °C -
Pré-séchage - temps 3 - 4 h -
Température de la matière fondue 250 - 300 °C -
Température du moule 70 - 90 °C -
Caractéristiques
Transformation
Moulage par injection
Caractéristiques
Bas gauchissement
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.