Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Beograde FLM013 T - PLA - Beologic nv

Material Data Center offers the following functions for Beograde FLM013 T:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Beograde datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 1190 MPa ISO 527
Contrainte d'écoulement 21 MPa ISO 527
Déformation au seuil d'écoulement 7.1 % ISO 527
Déformation à la rupture 140 % ISO 527
Module de flexion, 23°C 1030 MPa ISO 178
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 115 °C ISO 11357-1/-3
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1360 kg/m³ ISO 1183
Bulk density 800 kg/m³ -
Propriétés mécaniques (Grades film)ValeurUnitéNorme du test
ISO Data
Résistance à la déchirure Elmendorf, parallèle 1.69 N ISO 6383-2
Résistance à la déchirure Elmendorf, perpend. 0.42 N ISO 6383-2
Caractéristiques
Transformation
Extrusion de films
Conditionnement
Blanc
Propriétés spéciales
Transparent
Certifications
Contient des ressources renouvelables, Biodégradables
Disponibilité régionale
Europe, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.