Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CALIBRE™ 302EP-22 - PC - Trinseo

Material Data Center offers the following functions for CALIBRE™ 302EP-22:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Calibre datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité, MFI 22 g/10min ISO 1133
Température 300 °C -
Charge 1.2 kg -
Retrait au moulage, parallèle 0.6 % ISO 294-4, 2577
ASTM Data
Indice de fluidité, MFI 22 g/10min ASTM D 1238
Température 300 °C -
Charge 1.2 kg -
Retrait au moulage , parallèle 0.006 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2400 MPa ISO 527
Contrainte d'écoulement 60 MPa ISO 527
Déformation au seuil d'écoulement 6 % ISO 527
Contrainte à la rupture 65 MPa ISO 527
Déformation à la rupture >50 % ISO 527
Module de flexion, 23°C 2400 MPa ISO 178
Résistance au choc Charpy (entaillé), +23°C 20 kJ/m² ISO 179/1eA
Résistance au choc Izod avec entaille, +23°C 74 kJ/m² ISO 180/1A
ASTM Data
Module en traction 2344 MPa ASTM D 638
Module de traction d’élasticité 60 MPa ASTM D 638
Résistance de traction à la rupture 65.5 MPa ASTM D 638
Allongement d’élasticité 6 % ASTM D 638
Allongement à la rupture 120 % ASTM D 638
Module de flexion 2413 MPa ASTM D 790
Résistance à la flexion 96.5 MPa ASTM D 790
Dureté Rockwell R 118 - ASTM D 785
Izod choc avec entaille, 1/8 in 747 J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 122 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 147 °C ISO 306
Inflammabilité ep. nom. 1.5 mm V-2 class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 mm -
Inflammabilité pr. épaisseur h V-2 class IEC 60695-11-10
Epaisseur de l'éprouvette 3.2 mm -
Aptitude à l'allumage 26 % ISO 4589-1/-2
ASTM Data
UL 94 inflammabilité V-2 - UL 94
Épaisseur testée 1.59 mm -
coefficient de dilatation thermique, long. 68.4 E-6/K ASTM D 696
DTUL à 264 psi 126 °C ASTM D 648
Vicat température 147 °C ASTM D 1525
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Rigidité diélectrique 17 kV/mm IEC 60243-1
Indice de résistance au cheminement 250 - IEC 60112
ASTM Data
Rigidité diélectrique, peu de temps 16.5 kV/mm ASTM D 149
Facteur de dissipation diélectrique, 1 MHz 0.002 - ASTM D 150
Constante diélectrique, 60 Hz 3 - ASTM D 150
Constante diélectrique, 1 MHz 3 - ASTM D 150
Résistance volumique >1E15 Ohm*cm ASTM D 257
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Haze 1 % ASTM D 1003
Lumière á Transmittance 89 % ASTM D 1003
Indice de réfraction 1.59 - ASTM D 542
Propriétés diversesValeurUnitéNorme du test
Absorption d'humidité 0.32 % Sim. to ISO 62
Masse volumique 1200 kg/m³ ISO 1183
Absorption d’eau, 24hr 0.15 % ASTM D 570
Absorption d’eau, équilibre 0.32 % ASTM D 570
Densité 1200 kg/m³ ASTM D 792
Caractéristiques
Transformation
Moulage par injection
Propriétés spéciales
Modifié choc, Stabilisé aux intempéries, Stabilisé à la chaleur
Applications
Électrotechnique et électrique
Disponibilité régionale
Amérique du nord, Europe, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.