Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ChronoPrene™ 15A - TPE - AdvanSource Biomaterials

Material Data Center offers the following functions for ChronoPrene™ 15A:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Chronoprene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Indice de fluidité, MFI 14 g/10min ASTM D 1238
Température 200 °C -
Charge 5 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ASTM Data
Module de traction 7.58 MPa ASTM D 638
Allongement à la rupture 1820 % ASTM D 638
Dureté A Shore 15 - ASTM D 2240
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 71.1 - 93.3 °C -
Pré-séchage - temps 3 - 4 h -
L'humidité de traitement ≤0.05 % -
Zone 1 171 - 193 °C -
Zone 2 171 - 193 °C -
Zone 3 182 - 204 °C -
Température de la buse 171 - 193 °C -
Recommandations pour la transformation ExtrusionValeurUnitéNorme du test
Pré-séchage - température 71.1 - 93.3 °C -
Pré-séchage - temps 3 - 4 h -
L'humidité de traitement ≤0.05 % -
Zone 1 171 - 193 °C -
Zone 2 171 - 193 °C -
Zone 3 182 - 204 °C -
Température de la buse 171 - 193 °C -
Caractéristiques
Transformation
Moulage par injection, Extrusion (autres), Soufflage
Conditionnement
Granulés
Propriétés spéciales
Stabilisé aux intempéries
Résistance Chimique
Résistance chimique générale
Certifications
Contient des ressources renouvelables, Grade médical, Biocompatibility ISO 10993, USP Class VI approbation
Applications
Médical
Disponibilité régionale
Amérique du nord
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.