Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CirculenRenew C14 LD2420F Plus - (PE-LD) - LyondellBasell Industries

Material Data Center offers the following functions for CirculenRenew C14 LD2420F Plus:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Circulen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité, MFI 0.75 g/10min ISO 1133
Température 190 °C -
Charge 2.16 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 260 MPa ISO 527
Contrainte d'écoulement 11 MPa ISO 527
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 111 °C ISO 11357-1/-3
Température de ramolliss. Vicat, A 96 °C ISO 306
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Brillant 90 - ASTM D 2457
Haze 8 % ASTM D 1003
Propriétés diversesValeurUnitéNorme du test
Masse volumique 923 kg/m³ ISO 1183
Propriétés mécaniques (Grades film)ValeurUnitéNorme du test
ISO Data
Contrainte maximale, parallèle 26 MPa ISO 527-3
Contrainte maximale, perpend. 24 MPa ISO 527-3
Déformation maximale, parallèle 300 % ISO 527-3
Déformation maximale, perpend. 600 % ISO 527-3
Coefficient de friction dynamique 0.8 - ISO 8295
Type d'extrusion soufflage - -
Epaisseur des eprouvettes 0.05 mm -
Recommandations pour la transformation ExtrusionValeurUnitéNorme du test
Type of extrusion blown - -
Température de la matière fondue 170 - 220 °C -
Caractéristiques
Transformation
Extrusion a film soufflé, Extrusion de films
Conditionnement
Granulés
Caractéristiques
Soudage à la chaleur, Bas gel, Tenue de la matière à l’état fondu
Certifications
Contient des ressources renouvelables, Résine de contenu recyclé, Contact alimentaire
Applications
General Purpose, Emballage
Disponibilité régionale
Europe, Asia Pacific, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com