Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Denilen M 3031 - PP-(MF+GF)30 - VAMP TECH SPA

Material Data Center offers the following functions for Denilen M 3031:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Denilen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Retrait au moulage , parallèle 0.009 mm/mm ASTM D 955
Retrait au moulage, perpendiculaire 0.01 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Résistance au choc Izod, +23°C 15 kJ/m² ISO 180/1U
Résistance au choc Izod avec entaille, +23°C 5 kJ/m² ISO 180/1A
ASTM Data
Module en traction 4500 MPa ASTM D 638
Module de traction d’élasticité 35 MPa ASTM D 638
Allongement à la rupture 3 % ASTM D 638
Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
DTUL à 264 psi 125 °C ASTM D 648
Vicat température 115 °C ASTM D 1525
Propriétés diversesValeurUnitéNorme du test
Densité 1100 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 70 °C -
Pré-séchage - temps 3 h -
Température de la matière fondue 210 °C -
Température du moule 60 °C -
Caractéristiques
Transformation
Moulage par injection
Caractéristiques
Homopolymère
Disponibilité régionale
Europe
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.