Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Dielectrite 44-10 BMC - (Polyester+VE) - IDI Composites International

Material Data Center offers the following functions for Dielectrite 44-10 BMC:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Dielectrite datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Retrait au moulage , parallèle 0.002 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ASTM Data
Module de traction 41.4 MPa ASTM D 638
Résistance de compression 145 MPa ASTM D 695
Module de flexion 12410 MPa ASTM D 790
Résistance à la flexion 110 MPa ASTM D 790
Izod choc avec entaille, 1/8 in 240 J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Inflammabilité 5V pr. épaisseur h 5VA class IEC 60695-11-20
Epaisseur de l'éprouvette 1.9 mm -
ASTM Data
UL 94 inflammabilité V-0 - UL 94
Épaisseur testée 1.91 mm -
DTUL à 264 psi 260 °C ASTM D 648
Propriétés électriquesValeurUnitéNorme du test
ASTM Data
Résistance à l’arc 180 s ASTM D 495
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.15 % Sim. to ISO 62
Densité 1960 kg/m³ ASTM D 792
Caractéristiques
Transformation
Moulage par injection, Moulage par transfert, Moulage par compression
Conditionnement
Moulage en vrac
Propriétés spéciales
Ignifugé, Stabilisé aux intempéries
Caractéristiques
Stabilité de la couleur
Applications
General Purpose
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.