Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ BR003-30 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ BR003-30:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

Eastman Eastar™ Renew BR003-30 copolyester is a brilliantly clear copolyester for toothbrushes specifically designed for brands and manufacturers who demand a more sustainable plastic material. Eastar™ Renew BR003-30 copolyester is identical in clarity, resistance to toothpaste and mouthwash, and in processing ease to Eastar™ BR003, which oral care brands around the world have come to count on for their simple and complex toothbrush designs.

Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Renew polymers enable a brand to reduce consumption of fossil feedstock-based plastics, achieve sustainability targets without compromise, and be a fast mover in a growing market for sustainable consumer products.


Propriétés mécaniquesValeurUnitéNorme du test
ASTM Data
Module de flexion 2000 MPa ASTM D 790
Dureté Rockwell R 103 - ASTM D 785
Izod choc avec entaille, 1/8 in 80 J/m ASTM D 256
Izod choc avec entaille, bas température 40 J/m ASTM D 256
Température -40 °C -
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Haze 0.3 % ASTM D 1003
Lumière á Transmittance 91 % ASTM D 1003
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 70 °C -
Pré-séchage - temps 3 h -
Température de la matière fondue 230 - 280 °C -
Température du moule 15 - 30 °C -
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Couleurs naturelles
Propriétés spéciales
Transparent
Caractéristiques
Copolymère
Certifications
Contact alimentaire, FDA 21 CFR approbation, ISCC Plus
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.