Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ EN052 - Polyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ EN052:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

Eastar™ Polyester EN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystallized.





Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Retrait au moulage , parallèle 0.004 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ASTM Data
Module de traction d’élasticité 57 MPa ASTM D 638
Résistance de traction à la rupture 26 MPa ASTM D 638
Allongement d’élasticité 4 % ASTM D 638
Module de flexion 2500 MPa ASTM D 790
Dureté Rockwell R 110 - ASTM D 785
Izod choc avec entaille, 1/8 in 51 J/m ASTM D 256
Izod choc avec entaille, bas température 36 J/m ASTM D 256
Température -40 °C -
Résistance au choc Izod, 1/8 in N J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
DTUL à 66 psi 66 °C ASTM D 648
DTUL à 264 psi 62 °C ASTM D 648
Vicat température 79 °C ASTM D 1525
Propriétés électriquesValeurUnitéNorme du test
ASTM Data
Rigidité diélectrique, peu de temps 15.7 kV/mm ASTM D 149
Facteur de dissipation diélectrique, 1 MHz 0.02 - ASTM D 150
Constante diélectrique, 1 MHz 3 - ASTM D 150
Résistance de la surface 1E16 Ohm ASTM D 257
Résistance volumique 1E16 Ohm*cm ASTM D 257
Résistance à l’arc 155 s ASTM D 495
Propriétés diversesValeurUnitéNorme du test
Absorption d’eau, 24hr 0.1 % ASTM D 570
Densité 1320 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 150 - 160 °C -
Pré-séchage - temps 4 - 6 h -
Température de la matière fondue 275 - 295 °C -
Température du moule 10 - 30 °C -
Caractéristiques
Transformation
Moulage par injection
Caractéristiques
Homopolymère
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.