Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ EN067 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ EN067:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

Eastar™ Copolyester EN067 is a copolymer PET with good color. This product is supplied as a crystalline pellet that has improved flowability characteristics. Due to slower crystallization kinetics, this product is capable of producing a part free of crystalline haze upon injection molding. This product is tailored for the injection-molded cosmetics and personal care market.




Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Retrait au moulage , parallèle 0.0035 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ASTM Data
Module de traction d’élasticité 57 MPa ASTM D 638
Résistance de traction à la rupture 24 MPa ASTM D 638
Allongement d’élasticité 4 % ASTM D 638
Allongement à la rupture 134 % ASTM D 638
Module de flexion 2600 MPa ASTM D 790
Résistance à la flexion 81 MPa ASTM D 790
Dureté Rockwell 110 - ASTM D 785
Izod choc avec entaille, 1/8 in 58 J/m ASTM D 256
Izod choc avec entaille, bas température 29 J/m ASTM D 256
Température -40 °C -
Résistance au choc Izod, 1/8 in N J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
DTUL à 66 psi 66 °C ASTM D 648
DTUL à 264 psi 61 °C ASTM D 648
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Lumière á Transmittance 84 % ASTM D 1003
Propriétés diversesValeurUnitéNorme du test
Densité 1320 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 150 - 160 °C -
Pré-séchage - temps 4 - 6 h -
Température de la matière fondue 270 - 290 °C -
Température du moule 10 - 30 °C -
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Caractéristiques
Copolymère
Certifications
Contact alimentaire
Applications
Emballage
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.