Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Elastollan® 1154 D FHF - (TPU-ARET) - BASF Polyurethanes GmbH

Material Data Center offers the following functions for Elastollan® 1154 D FHF:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Elastollan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
DESCRIPTION
Elastollan 1154 D FHF is a halogen free, flame retarded polyether based TPU

SPECIAL PROPERTIES
excellent resistance to hydrolysis and good flexibility at low temperature,
resistance to microbiological attack, good wear performance,
high tensile strength, good damping behavior

TYPICAL APPLICATIONS
cable sheathing, hoses, profiles

OTHER HINTS
predrying: 2-3h at 100-110°C,
max. content of humidity before processing: 0,02%
annealing: 20 h at 100°C in order to get optimum properties

CHEMICAL RESISTANCE
For detailed information on the chemical resistance of our
materials refer to this list of chemical resistance
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 160 MPa ISO 527
Résistance au choc Charpy (entaillé), +23°C 50 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 3 kJ/m² ISO 179/1eA
Contrainte à 100% de déformation 19 MPa ISO 527
Contrainte à 300% de déformation 33 MPa ISO 527
Contrainte à la rupture TPE 30 MPa ISO 527
Déformation à la rupture TPE >300 % ISO 527
Déformation rémanente en compression à 23 °C, 24h 30 % ISO 815
Déformation rémanente en compression à 70 °C, 24h 45 % ISO 815
Résistance à la déchirure 110 kN/m ISO 34-1
Résistance à l'abrasion 40 mm³ ISO 4649
Dureté Shore D 55 - ISO 7619-1
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Inflammabilité ep. nom. 1.5 mm V-0 class IEC 60695-11-10
Yellow Card disponible oui - -
Inflammabilité pr. épaisseur h V-0 class IEC 60695-11-10
Epaisseur de l'éprouvette 3.0 mm -
Yellow Card disponible oui - -
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1270 kg/m³ ISO 1183
Fonctions
Viscosité / Vitesse de cisaillement , Elastollan® 1154 D FHF, (TPU-ARET), BASF PU
Contrainte de cisaillement / Vit. de cisaillement , Elastollan® 1154 D FHF, (TPU-ARET), BASF PU
Module de cisaillement dynamique / Température , Elastollan® 1154 D FHF, (TPU-ARET), BASF PU
Contrainte / Déformation (TPE) , Elastollan® 1154 D FHF, (TPU-ARET), BASF PU
Caractéristiques
Transformation
Moulage par injection, Extrusion de profilés
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.