Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of FLEXIRENE® MS 20 A - (PE-LLD) - Versalis S.p.A

Material Data Center offers the following functions for FLEXIRENE® MS 20 A:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Flexirene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Polyéthylène linear basse densité avec antioxydants, mis au point pour le moulage par injection.
Flexirene MS 20 A a une tenue élevée à basse temperature.

Applications
Rècipients pour détergens, bouchons pour produits chimiques, rècipients pour basse température, mélanges maîtres pour LLDPE et LDPE. 
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 26 cm³/10min ISO 1133
Température 190 °C -
Charge 2.16 kg -
Densité du fondu 746 kg/m³ -
Conductivité thermique du fondu 0.39 W/(m K) -
Chaleur spécifique du fondu 2810 J/(kg K) -
Température d'éjection 83 °C -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 150 MPa ISO 527
Contrainte pr. une déform. de 50% 10 MPa ISO 527
Déformation à la rupture >50 % ISO 527
Dureté Shore D 48 - ISO 7619-1
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 113 °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min 101 °C ISO 11357-1/-2
Coeffic. de dilatation therm. linéique, parallèle 152 E-6/K ISO 11359-1/-2
Propriétés diversesValeurUnitéNorme du test
Masse volumique 921 kg/m³ ISO 1183
Fonctions
Viscosité / Vitesse de cisaillement , FLEXIRENE® MS 20 A, (PE-LLD), Versalis
Contrainte de cisaillement / Vit. de cisaillement , FLEXIRENE® MS 20 A, (PE-LLD), Versalis
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Autres informations
Moulages par injection

#2

Conditions typiques de transformation:

    Température matière         160 - 210 °C

    Température du moule        10 -  40  °C

Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.