Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of FORTRON® LM1140L4 - PPS-GF40 - Celanese

Material Data Center offers the following functions for FORTRON® LM1140L4:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Fortron datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Fortron LM1140L4 is a 40% glass-reinforced grade that is the strongest and toughest product available. It is laser markable.  It exhibits excellent heat and chemical resistance, good electrical properties and is inherently flame-retardant. The high hardness and rigidity at elevated temperatures allows for good load bearing performance. This product has good weldability due to the modest filler level. Applications made of this grade are electronical components (i.e. bobbins, lamp housings, brush holders) and various other components requiring strength and resistance to aggressive chemicals (i.e. automotive heaters, pumps, valves, fuel rails, microwave oven rings and distillation column packings).

Flammability @1.6mm nom. thickn.V-0-
Flammability at thickness h (0.38 mm)V-0-
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Retrait au moulage, parallèle 0.3 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.6 % ISO 294-4, 2577
Chaleur spécifique du fondu 1500 J/(kg K) -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 14700 MPa ISO 527
Contrainte à la rupture 195 MPa ISO 527
Déformation à la rupture 1.9 % ISO 527
Résistance au choc Charpy, +23°C 53 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 53 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 10 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 10 kJ/m² ISO 179/1eA
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 280 °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min 90 °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 270 °C ISO 75-1/-2
Température de fléchissement s/chrg, 8.00 MPa 215 °C ISO 75-1/-2
Coeffic. de dilatation therm. linéique, parallèle 26 E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 42 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm V-0 class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 mm -
Inflammabilité pr. épaisseur h V-0 class IEC 60695-11-10
Epaisseur de l'éprouvette 0.4 mm -
Inflammabilité 5V pr. épaisseur h 5VA class IEC 60695-11-20
Epaisseur de l'éprouvette 3.0 mm -
Aptitude à l'allumage 47 % ISO 4589-1/-2
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 1MHz 4.1 - IEC 62631-2-1
Facteur de pertes, 1MHz 20 E-4 IEC 62631-2-1
Résistivité transversale >1E13 Ohm*m IEC 62631-3-1
Résistivité superficielle 6.6E11 Ohm IEC 62631-3-2
Rigidité diélectrique 28 kV/mm IEC 60243-1
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.02 % Sim. to ISO 62
Masse volumique 1650 kg/m³ ISO 1183
Fonctions
Module de cisaillement dynamique / Température , FORTRON® LM1140L4, PPS-GF40, Celanese
Contrainte / Déformation , FORTRON® LM1140L4, PPS-GF40, Celanese
Module sécant / Déformation , FORTRON® LM1140L4, PPS-GF40, Celanese
Contrainte / Déformation (isochrone) 23°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Module de fluage / Temps 23°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Courbe de fluage 23°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Contrainte / Déformation (isochrone) 120°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Module de fluage / Temps 120°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Courbe de fluage 120°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Contrainte / Déformation (isochrone) 150°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Module de fluage / Temps 150°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Courbe de fluage 150°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Contrainte / Déformation (isochrone) 200°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Module de fluage / Temps 200°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Courbe de fluage 200°C, FORTRON® LM1140L4, PPS-GF40, Celanese
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Additifs
Agent de démoulage
Autres informations
Moulages par injection
Predrying in a dehumidified air dryer at 130 - 140 degC/3-4 hours is recommended.
On injection molding machines with 15-25 D long three-section screws, as are usual in the trade, the FORTRON is processable. A shut-off nozzle is preferred to a free-flow nozzle.

Melt temperature 320-340 degC
Mold wall temperature at least 140 degC

A medium injection rate is normally preferred. All mold cavities must be effectively vented.
Tool temperature of at least 135 degC is recommended for parts to achieve maximum crystallizable potential.
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.