Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Hybrid S555 - (PC+ABS) - Ravago Manufacturing Americas

Material Data Center offers the following functions for Hybrid S555:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Hybrid S datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 24 cm³/10min ISO 1133
Température 260 °C -
Charge 2.16 kg -
Retrait au moulage, parallèle 0.6 % ISO 294-4, 2577
ASTM Data
Indice de fluidité, MFI 21 g/10min ASTM D 1238
Température 260 °C -
Charge 2.16 kg -
Retrait au moulage , parallèle 0.006 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Contrainte d'écoulement 62 MPa ISO 527
Déformation à la rupture 48 % ISO 527
Module de flexion, 23°C 2550 MPa ISO 178
Résistance au choc Izod avec entaille, +23°C 44 kJ/m² ISO 180/1A
ASTM Data
Module de traction d’élasticité 63.4 MPa ASTM D 638
Allongement à la rupture 45 % ASTM D 638
Module de flexion 2550 MPa ASTM D 790
Résistance à la flexion 84.1 MPa ASTM D 790
Izod choc avec entaille, 1/8 in 640 J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 91 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 105 °C ISO 75-1/-2
Inflammabilité 5V pr. épaisseur h 5VB class IEC 60695-11-20
Epaisseur de l'éprouvette 2.5 mm -
ASTM Data
UL 94 inflammabilité V-0 - UL 94
Épaisseur testée 1.5 mm -
DTUL à 66 psi 107 °C ASTM D 648
DTUL à 264 psi 93.9 °C ASTM D 648
Vicat température 110 °C ASTM D 1525
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1180 kg/m³ ISO 1183
Densité 1180 kg/m³ ASTM D 792
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Propriétés spéciales
Ignifugé
Disponibilité régionale
Amérique du nord
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.